Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 52 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 52 g/10 min

@Load 2.16 kg,
Temperature 190 °C
52 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Procedure A Condition E; ASTM D1238
Network Polymers Kepital® F40-03
Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc.
Melt Flow 52 g/10 min

@Load 2.16 kg,
Temperature 190 °C
52 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
NOVA Chemicals Sclair® 2114 LLDPE Injection Molding Resin
Features: High stiffness, high impact strength and low warpage, good top loading capability, high surface gloss.Applications: Container (tub) lids and closures.Data provided by the manufacturer.
Melt Flow 52 g/10 min

@Load 2.16 kg,
Temperature 190 °C
52 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Procedure A; ASTM D1238
PolyOne Elastamax™ EG-9065 Thermoplastic Elastomer (TPE)
The Elastamax™ EG 9000 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9000 Series of compoun..
Melt Flow 52 g/10 min

@Load 10.0 kg,
Temperature 220 °C
52 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
LG Chemical AF312 ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical..
Melt Flow 52 g/10 min

@Load 10.0 kg,
Temperature 220 °C
52 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
LG Chemical AF312T ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical..
Melt Flow 52 g/10 min
52 g/10 min
Intercontinental Polymers HoPBT 303 HoPBT Polymer Type - Clear, Polyester Pellets
Applications: Engineering Resin Information provided by Intercontinental Polymers.
Melt Flow 52 g/10 min

@Load 5.00 kg,
Temperature 260 °C
52 g/10 min

@Load 11.0 lb,
Temperature 500 °F
Estimated using room temperature density; ISO 1133
Lanxess Durethan® BKV 15 G H2.0 900051 Copolyamide, 15% Glass Fiber
CoPA, injection molding grade, 15% glass fibers, better surface resistance to alcoholic calcium chloride-solution than BKV 15 H2.0, good heat-ageing resistance
Melt Flow 52 g/10 min

@Load 5.00 kg,
Temperature 250 °C
52 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics Valox® IQ420 PBT
Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc.
Melt Flow 52 g/10 min

@Load 5.00 kg,
Temperature 250 °C
52 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics Valox® IQ420 PBT (Asia Pacific)
Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc.
Melt Flow 52 g/10 min

@Load 5.00 kg,
Temperature 250 °C
52 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics Valox® IQ420 PBT (Europe-Africa-Middle East)
Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc.
Melt Flow 52 g/10 min

@Load 5.00 kg,
Temperature 250 °C
52 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics Valox® IQ420HP PBT (Asia Pacific)
Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production..
Melt Flow 52 g/10 min

@Load 10.0 kg,
Temperature 220 °C
52 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Samsung Cheil Industries Starex® NH-1904 HIPS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Melt Flow 52 g/10 min

@Load 10.0 kg,
Temperature 220 °C
52 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Samsung Cheil Industries Starex® NH-1904 HIPS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Melt Flow 52 g/10 min

@Load 5.00 kg,
Temperature 250 °C
52 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics Valox® IQ420HP PBT
Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production..
Melt Flow 52 g/10 min

@Load 5.00 kg,
Temperature 250 °C
52 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics Valox® IQ420HP PBT (Europe-Africa-Middle East)
Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production..
Melt Flow 52 g/10 min

@Load 2.16 kg,
Temperature 224 °C
52 g/10 min

@Load 4.76 lb,
Temperature 435 °F
ASTM D1238
DSM Biomedical CarboSil® 20 80A Thermoplastic Silicone Polycarbonate Polyurethane (TSPCU)
A ground-breaking copolymer that combines the biocompatibility and biostability of conventional silicone elastomers with the processability and toughness of thermoplastic polycarbonate-urethanes Th..
Melt Flow 52 g/10 min

@Load 2.16 kg,
Temperature 190 °C
52 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil LL 5252.09 Compounding Resin
Product Description: LL 5252.09 is a linear low density polyethylene resin designed to provide good processability and ease of blending. The granular from of LL 5252.09 makes for efficient blending ..
Melt Flow 52 g/10 min

@Load 2.16 kg,
Temperature 190 °C
52 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil LLDPE LL 5252.09 Linear Low Density Polyethylene Resin
Product Description: LL 5252.09 is a linear low density polyethylene resin designed to provide good processability and ease of blending. The granular from of LL 5252.09 makes for efficient blending ..
Melt Flow 52 g/10 min

@Load 2.16 kg,
Temperature 250 °C
52 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ISO 1133
BASF Ultradur B 2550 PBT
Ultradur B2550 is an unfilled, very free-flowing grade for coating paper and board with high heat resistance, for example for packaging of frozen goods and ready-prepared meals. Also suitable for in..
Copyright © lookpolymers.com All Rights Reserved