Product Description: LD 151 series LDPE grades offer an excellent combination of high clarity with high stiffness. Several additive packages are available according to the required surface properties.Availability: Africa & Middle East and Europe Additive: Antiblock: 1000 ppmSlip: 1050 ppmThermal Stabilizer: YesApplications: Cast FilmCo-Extrusion FilmsEmbossed FilmHygiene PackagingLabel FilmOverwrap FilmPaper OverwrapInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.934 g/cc
0.0337 lb/in³
ExxonMobil method
Melt Flow 3.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Antiblock Level 1000 ppm
1000 ppm
Slip Level 1050 ppm
1050 ppm
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 17.2 MPa
2500 psi
ASTM D882
Film Elongation at Break, MD 370 %
370 %
ASTM D882
Film Elongation at Break, TD 610 %
610 %
ASTM D882
Elmendorf Tear Strength MD 90 g
90 g
ASTM D1922
Elmendorf Tear Strength TD 180 g
180 g
ASTM D1922
Dart Drop Test 60.0 g
0.132 lb
ASTM D1709A
Film Tensile Strength at Break, MD 26.2 MPa
3800 psi
ASTM D882
Film Tensile Strength at Break, TD 20.7 MPa
3000 psi
ASTM D882
1% Secant Modulus, MD 379 MPa
55000 psi
ASTM D882
1% Secant Modulus, TD 441 MPa
64000 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point <= 241 °C
<= 466 °F
Peak Melting Point; ExxonMobil method
Optical Properties Metric English Comments
Haze 6.0 %
6.0 %
ASTM D1003
Gloss 73 %
73 %
45°; ASTM D2457
Users viewing this material also viewed the following: