Mechanical Properties Metric English Comments
Elmendorf Tear Strength TD 180 g
180 g
Eastman E6838-997F Polyethylene  (discontinued **)
E6838-997F natural is a low density formulation with no slip or antiblock. Outstanding optical properties make this material an excellent choice for calendering and as a clarity filler in co-extrud..
Elmendorf Tear Strength TD 180 g
180 g
ASTM D1922
ExxonMobil LD 135.09 Blown Film Resin  (discontinued **)
LD 135.09 is a homopolymer film resin with good clarity. Applications include food packaging, light to medium duty bags, and textile packaging.Information provided by ExxonMobil Chemical
Elmendorf Tear Strength TD 180 g
180 g
ASTM D1922
ExxonMobil LD 145.PX Packaging Resin  (discontinued **)
LD 145.PX resin is a homopolymer cast film resin offering good clarity and toughness. Applications include Bread bags and other Food Packaging.Information provided by ExxonMobil Chemical
Elmendorf Tear Strength TD 180 - 520 g
180 - 520 g
Average value: 351 g Grade Count:20
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Butene, Film
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Butene, Film". Each property range of values reported is minimum..
Elmendorf Tear Strength TD 180 g
180 g
ASTM D1922
LyondellBasell Petrothene® GA503027 Linear Low Density Polyethylene (0.5 mil Film)
ApplicationsGA 503 is a medium density, butene copolymer LLDPE resin with high draw for stiff, thin blown films. GA 503 contains an antioxidant package to minimize discoloration and eliminate die b..
Elmendorf Tear Strength TD 180 g
180 g
ASTM D1922
LyondellBasell Petrothene® NA442051 Low Density Polyethylene
ApplicationsPETROTHENE NA 442 is a series of low density/EVA copolymer resins for high impact/high clarity packaging and lamination applications. NA 442 exhibits excellent processability and good b..
Elmendorf Tear Strength TD 180 g
180 g
ASTM D1922
LyondellBasell Petrothene® NA963083 Low Density Polyethylene
ApplicationsPETROTHENE NA 963 is a series of resins formulated with special antiblock additive and designed for a wide variety of industrial film applications where high impact strength and excellen..
Elmendorf Tear Strength TD 180 g
180 g
ASTM D1922
LG Chemical SEETEC BF410 LDPE
Characteristics: Good Processability and Excellent Optical PropertiesAdditives: Antiblocking Agent, Slip AgentApplications: Industrial Film & Food PackageCAS No. 9002-88-4Information provided by LG ..
Elmendorf Tear Strength TD 180 g
180 g
ASTM D1922
LG Chemical SEETEC BF415 LDPE
Characteristics: Good Processability and Excellent Optical Properties Applications: Masking filmCAS No. 9002-88-4Information provided by LG Chemical
Elmendorf Tear Strength TD 180 g
180 g
ASTM D1922
LG Chemical SEETEC BF500 LDPE
Characteristics: Good Processability and Good Optical Properties Additives: Antiblocking Agent, Slip AgentApplications: Industrial Film & Food PackageCAS No. 9002-88-4Information provided by LG Chem..
Elmendorf Tear Strength TD 180 g
180 g
ASTM D1922
ExxonMobil LD 105.30 Very High Clarity Packaging Film Resin
Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or..
Elmendorf Tear Strength TD 180 g
180 g
ASTM D1922
ExxonMobil LDPE LD 105.30 Low Density Polyethylene Resin
Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or..
Elmendorf Tear Strength TD 180 g
180 g
ASTM D1922
ExxonMobil LDPE LD 105.BR Low Density Polyethylene Resin
Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or..
Elmendorf Tear Strength TD 180 g
180 g
ASTM D1922
ExxonMobil LDPE LD 151BW Low Density Polyethylene Resin
Product Description: LD 151 series LDPE grades offer an excellent combination of high clarity with high stiffness. Several additive packages are available according to the required surface propertie..
Elmendorf Tear Strength TD 180 g
180 g
ASTM D1922
ExxonMobil LDPE LD 151GZ Low Density Polyethylene Resin
Product Description: LD 151 series LDPE grades offer an excellent combination of high clarity with high stiffness. Several additive packages are available according to the required surface propertie..
Elmendorf Tear Strength TD 180 g
180 g
ASTM D1922
ExxonMobil LDPE LD 151HR Low Density Polyethylene Resin
Product Description: LD 151 series LDPE grades offer an excellent combination of high clarity with high stiffness. Several additive packages are available according to the required surface propertie..
Elmendorf Tear Strength TD 180 g
180 g
ASTM D1922
ExxonMobil LDPE LD 364HE Low Density Polyethylene Resin
Product Description: LD 364HE is an LDPE, offering a good combination of mechanical, optical and sealing properties.Availability: Africa & Middle East and Europe Additive: Antiblock: 1500 ppmSlip: ..
Elmendorf Tear Strength TD 180 g
180 g
ASTM D1922
ExxonMobil LDPE LD 380BA Blown Low Density Polyethylene Resin (European Grade)
Product Description: LD 380BA offers good toughness and optical properties.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: NoApplications: Coextrus..
Elmendorf Tear Strength TD 180 g
180 g
ASTM-D1922
Braskem FP33 LLDPE Blown Film Extrusion Polyethylene Copolymer
The FP33 resin is a linear low-density polyethylene, copolymer of butene-1, produced by the solution process for film extrusion with good mechanical properties. It contains processing aid, slip, and..
Elmendorf Tear Strength TD 180 g
180 g
ASTM D1922
3M 6142 Medium Duty Water Activated Paper Tape
3M™ Medium Duty Water Activated Paper Tape 6142 is used for box sealing and other packaging applications. This product has a paper backing and a gummed, high tack, water-activated, modified cornsta..
Elmendorf Tear Strength TD 180 g
180 g
ASTM D1922
ExxonMobil Escorene™ FL 00218 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: FL 00218 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 240°C (464°F) may cause resin degradation. Machines should always b..