Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 441 MPa | 64000 psi | ASTM D882 |
ExxonMobil LDPE LD 151BW Low Density Polyethylene Resin Product Description: LD 151 series LDPE grades offer an excellent combination of high clarity with high stiffness. Several additive packages are available according to the required surface propertie.. |
|||
1% Secant Modulus, TD | 441 MPa | 64000 psi | ASTM D882 |
ExxonMobil LDPE LD 151GZ Low Density Polyethylene Resin Product Description: LD 151 series LDPE grades offer an excellent combination of high clarity with high stiffness. Several additive packages are available according to the required surface propertie.. |
|||
1% Secant Modulus, TD | 441 MPa | 64000 psi | ASTM D882 |
ExxonMobil LDPE LD 151HR Low Density Polyethylene Resin Product Description: LD 151 series LDPE grades offer an excellent combination of high clarity with high stiffness. Several additive packages are available according to the required surface propertie.. |