Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 20.7 MPa | 3000 psi | ASTM D882 |
ExxonMobil LD 102.74 Thin Gauged Film Resin
(discontinued **) LD 102 series are homopolymer, good clarity, laundry and dry cleaning film resins capable of providing a tough film in very thin gaugesInformation provided by ExxonMobil Chemical |
|||
Film Tensile Strength at Break, TD | 20.7 MPa | 3000 psi | ASTM D882 |
ExxonMobil LD 103.MP Industrial Film Resin
(discontinued **) LD 103 resins are homopolymer industrial film resins are used in box and drum liners, industrial packaging, medium duty shrink wrap, construction and agriculture film, and rubber bale wrap.Informati.. |
|||
Film Tensile Strength at Break, TD | 20.7 - 27.6 MPa | 3000 - 4000 psi | ASTM D882 |
Honeywell ACLAR® 33C (7.80 mil) Copolymer Film
(discontinued **) Description: ACLAR® 33C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). 33C is used for military and industrial packaging applications.Information provided by Honeywell.. |
|||
Film Tensile Strength at Break, TD | 20.7 - 34.5 MPa | 3000 - 5000 psi | ASTM D882 |
Honeywell ACLAR® 33C (0.75 mil) Copolymer Film
(discontinued **) Description: ACLAR® 33C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). 33C is used for military and industrial packaging applications.Information provided by Honeywell.. |
|||
Film Tensile Strength at Break, TD | 20.7 MPa | 3000 psi | ASTM D882 |
LyondellBasell Petrothene® NA272130 Medium Density Polyethylene, Film Extrusion Grade PETROTHENE NA272130 is a medium density polyethylene resin designed for overwrap film applications. NA272130 exhibits good film optics and high stiffness.Regulatory Status: NA272130 meets the requir.. |
|||
Film Tensile Strength at Break, TD | 20.7 MPa | 3000 psi | ASTM D882 |
LyondellBasell Petrothene® NA480145 Low Density Polyethylene ApplicationsPETROTHENE NA 480 is a series of low density/EVA copolymer resins designed for specialty films. NA 480 produces film with superior puncture resistance, Heat sealability, clarity and low.. |
|||
Film Tensile Strength at Break, TD | 20.7 MPa | 3000 psi | ASTM D882 |
LyondellBasell Petrothene® NA480177 Low Density Polyethylene ApplicationsPETROTHENE NA 480 is a series of low density/EVA copolymer resins designed for specialty films. NA 480 produces film with superior puncture resistance, Heat sealability, clarity and low.. |
|||
Film Tensile Strength at Break, TD | 20.7 MPa | 3000 psi | ASTM D882 |
LyondellBasell Petrothene® NA480178 Low Density Polyethylene ApplicationsPETROTHENE NA 480 is a series of low density/EVA copolymer resins designed for specialty films. NA 480 produces film with superior puncture resistance, Heat sealability, clarity and low.. |
|||
Film Tensile Strength at Break, TD | 20.7 MPa | 3000 psi | ASTM D882 |
LG Chemical LUTENE FB0800 LDPE Blown Film Description: LUTENE FB0800 is mainly intended for the extrusion of blown film with high mechanical property for the manufacture of greenhouse film. LUTENE FB0800 have the excellent mechanical proper.. |
|||
Film Tensile Strength at Break, TD | 20.7 MPa | 3000 psi | D638 |
Westlake EF524 14.5% Ethylene Vinyl Acetate Copolymer Westlake ELEVATE™ EF524 is an ethylene vinyl acetate copolymer with 14.5% VA. EF524 is designed for blown and
cast films requiring excellent optics and low heat seal initiation. High melt strength.. |
|||
Film Tensile Strength at Break, TD | 20.7 MPa | 3000 psi | ASTM D638 |
Westlake Elevate™ EF598 9% Ethylene Vinyl Acetate Copolymer Westlake EF437 resin is a 2.5% EVA copolymer designed for films that require excellent optical and strength properties. This Kosher compliant resin has excellent heat sealing characteristics and low.. |
|||
Film Tensile Strength at Break, TD | 20.7 MPa | 3000 psi | ASTM D638 |
Westlake EMAC® EF598AA 9% Ethylene-Methyl Acrylate Copolymer Clarity optics, excellent drawdown, excellent machinability, good TD heat shrinkage and excellent toughness. Uses include food packaging tie layers, heat seal layers, extrusion coating, cast film, .. |
|||
Film Tensile Strength at Break, TD | 20.7 MPa | 3000 psi | ASTM D882 |
ExxonMobil LD 102.LC Thin Gauged Film Resin L Product Description: LD 102.LC is a formulated homopolymer, garment film resin with good toughness. It is capable of being drawndown to thing gauges.Availability: Latin America, North America and .. |
|||
Film Tensile Strength at Break, TD | 20.7 MPa | 3000 psi | ASTM D882 |
ExxonMobil LD 141.87 Shrink Film Resin LD 141.87 is a vinyl acetate copolymer film resin with very good toughness and shrink properties. Applications include Medium duty shrink wrap and Heavy duty bags.Information provided by ExxonMobil.. |
|||
Film Tensile Strength at Break, TD | 20.7 MPa | 3000 psi | ASTM D882 |
ExxonMobil LD 144.50 Packaging Film Resin Film made from LD 144.50 offers improved impact strength and heat sealability compared to homopolymer clarity film resins. Typically applications include food packaging, frozen food packaging, and .. |
|||
Film Tensile Strength at Break, TD | 20.7 MPa | 3000 psi | ASTM D882 |
ExxonMobil LDPE LD 151BW Low Density Polyethylene Resin Product Description: LD 151 series LDPE grades offer an excellent combination of high clarity with high stiffness. Several additive packages are available according to the required surface propertie.. |
|||
Film Tensile Strength at Break, TD | 20.7 MPa | 3000 psi | ASTM D882 |
ExxonMobil LDPE LD 151GZ Low Density Polyethylene Resin Product Description: LD 151 series LDPE grades offer an excellent combination of high clarity with high stiffness. Several additive packages are available according to the required surface propertie.. |
|||
Film Tensile Strength at Break, TD | 20.7 MPa | 3000 psi | ASTM D882 |
ExxonMobil LDPE LD 151HR Low Density Polyethylene Resin Product Description: LD 151 series LDPE grades offer an excellent combination of high clarity with high stiffness. Several additive packages are available according to the required surface propertie.. |
|||
Film Tensile Strength at Break, TD | 20.7 MPa | 3000 psi | ASTM D882 |
ExxonMobil LDPE LD 158BW Low Density Polyethylene Resin Product Description: LD 158 series are LDPE grades, specially designed for lamination and co-extruded films. They offer good mechanical, stiffness and optical properties, combined with very low gel .. |
|||
Film Tensile Strength at Break, TD | 20.7 MPa | 3000 psi | ASTM D882 |
ExxonMobil LDPE LD 158JD Low Density Polyethylene Resin Product Description: LD 158 series are LDPE grades, specially designed for lamination and co-extruded films. They offer good mechanical, stiffness and optical properties, combined with very low gel .. |
|||
Film Tensile Strength at Break, TD | 20.7 MPa | 3000 psi | ASTM D882 |
ExxonMobil LDPE LD 159AC Low Density Polyethylene Resin Product Description: LD 159AC is an LDPE grade, which offers good draw down combined with good mechanical strength. Availability: Africa & Middle East and Europe Additive: Antiblock: 450 ppmSlip: 5.. |
|||
Film Tensile Strength at Break, TD | 20.7 MPa | 3000 psi | ASTM D882 |
ExxonMobil Optema® TC-110 Blown Ethylene Methyl Acrylate Product Description: Optema TC 110 is an ethylene methyl acrylate copolymer specifically formulated to offer extrusion and property performance for blown film applications. It produces a soft, elast.. |
|||
Film Tensile Strength at Break, TD | 20.7 MPa | 3000 psi | ASTM D-882 |
Bapolene® 222F Polyethylene, Film Grade Bapolene LL222F is a general purpose LLDPE for blown film extrusion or cast film applications. This resin offers excellent tensile and toughness properties. It is available with and without slip/a.. |