ExxonMobil HDPE HMA 018 High Density Polyethylene Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Exxon Chemical
Trade Name HDPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil HDPE HMA 018 High Density Polyethylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: HMA 018 is an easy flow HDPE grade, characterized by high gloss and dimensional stability. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Thermal Stabilizer: YesUV Stabilizer: NoApplications: Food Packaging ContainersHousewares – Multicavity Thin-WalledInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.954 g/cc
0.0345 lb/in³
ASTM D4883
ESCR 10% Igepal® <= 1.0 hour

@Temperature 50.0 °C
<= 1.0 hour

@Temperature 122 °F
F50; ASTM D1963
Melt Flow 30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.1 MPa
3200 psi
ISO 527-2/1A/50
Elongation at Break >= 100 %
>= 100 %
ISO 527-2/1A/50
Elongation at Yield 10 %
10 %
ISO 527-2/1A/50
Flexural Modulus 0.896 GPa
130 ksi
ISO 178
Izod Impact, Notched (ISO) 3.78 kJ/m²
1.80 ft-lb/in²
ISO 180/1A
Thermal Properties Metric English Comments
Melting Point <= 264 °C
<= 507 °F
Peak Melting Point; ExxonMobil method
Deflection Temperature at 0.46 MPa (66 psi) 63.9 °C
147 °F
ISO 75-2/B
Users viewing this material also viewed the following: