Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 3.78 kJ/m² | 1.80 ft-lb/in² | ISO 180/1A |
ExxonMobil HDPE HMA 018 High Density Polyethylene Resin Product Description: HMA 018 is an easy flow HDPE grade, characterized by high gloss and dimensional stability. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Thermal Stabili.. |