Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.954 g/cc | 0.0345 lb/in³ | ASTM D1505 |
Petromont 3101 High Density Polyethylene Resin Petromont HDPE 3101 is a high density polyethylene resin produced using the UNIPOL® Process. This resin is intended for a broad range of injection moulding applications including open-head pails, h.. |
|||
Density | 0.954 g/cc | 0.0345 lb/in³ | ISO 1183 |
Yparex 8305 Polyolefin Adhesive Resin (European Grade)
(discontinued **) The Yparex range provides outstanding adhesion for all forms of polyethylene including cross-linked PE to: barrier plastics like EVOH and Polyamidemetals like aluminum, steel and copper.Yparex offer.. |
|||
Density | 0.954 g/cc | 0.0345 lb/in³ | ASTM D1505 |
SABIC M300054 High Density Polyethylene for Injection Molding Product Description: M300054 is a high density polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to provide good flow.. |
|||
Density | 0.954 g/cc | 0.0345 lb/in³ | ASTM D1505 |
Chevron Phillips Marlex® HXM TR-570 High Density Polyethylene
(discontinued **) High Density PolyethyleneCustomer Benefits: This extra high molecular weight polyethylene is tailored for large containers with exhibit outstanding impact and creep resistance, excellent ESCR, and e.. |
|||
Density | 0.954 g/cc | 0.0345 lb/in³ | |
LyondellBasell Lupolen® 5261 Z HDPE, Blow Molding Grade Relatively high viscosity blow molding grade for rigid, stackable and highly shock resistant containers for packaging all types of hazardous materials such as flammable, corrosive, poisonous and sur.. |
|||
Density | 0.954 g/cc | 0.0345 lb/in³ | |
LyondellBasell Lupolen® 5261 Z HI HDPE Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Density | 0.954 g/cc | 0.0345 lb/in³ | ASTM D1505 |
LyondellBasell Alathon® L5440 High Density Polyethylene ApplicationsALATHON L 5440 is designed for high shear machines. It exhibits excellent color, low odor and excellent processing stability. Typical applications include general purpose, household ch.. |
|||
Density | 0.954 g/cc | 0.0345 lb/in³ | ASTM D1505 |
LyondellBasell Lupolen® 5261 Z Q 456 High Density Polyethylene, Pipe and Sheet Extrusion Grade Lupolen 5261 Z Q 456 is a high density polyethylene (HDPE) with high melt viscosity for ram extrusion of peroxide crosslinked pipes (PE-Xa). The product is supplied as a nominal 20 mesh (840 µm) .. |
|||
Density | 0.954 g/cc | 0.0345 lb/in³ | |
JPJ Technologies 6360M HDPE Extrusion Information provided by JPJ Technologies |
|||
Density | 0.954 g/cc | 0.0345 lb/in³ | |
JPJ Technologies 700F HDPE Extrusion Information provided by JPJ Technologies |
|||
Density | 0.954 g/cc | 0.0345 lb/in³ | ASTM D792 |
Techmer ES HiFill® HDPE 8904 UV GY Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV ResistanceAppearance: GreyInformation provided by TP Composites, Inc. |
|||
Density | 0.954 g/cc | 0.0345 lb/in³ | ISO 1872/1 |
SIDPEC EGYPTENE® HD 5420 GA HDPE Blow Molding Applications:Large blow molded containers for applications which require maximum toughness220 liter drums for chemicalsInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Pe.. |
|||
Density | 0.954 g/cc | 0.0345 lb/in³ | DIN 53479/ASTM D1505 |
Silon Taborex TA 1131 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1131 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Density | 0.954 g/cc | 0.0345 lb/in³ | ISO 1183 |
Borealis Borstar® HE3496-LS Yellow Polyethylene Compound for The Coextrusion of Identifying Stripes On Black HD Pipe for Natural Gas Borstar HE3496-LS is a bimodal, cadmium free, high density polyethylene compound designed for coextrusion of blue identifying stripes. It is fully stabilized against thermal degradation and the die.. |
|||
Density | 0.954 g/cc | 0.0345 lb/in³ | ISO 1183 |
Borealis MG7547S Polyethylene MG7547S is a high-density polyethylene produced by a low pressure process. This grade has an excellent impact strength and low distortion even at low temperatures. It also contains UV stabilizer, wh.. |
|||
Density | 0.954 g/cc | 0.0345 lb/in³ | ISO 1183 |
Unipetrol PE HD LITEN® MB/ML 67 HDPE Made for injection molding applications.Information provided by Unipetrol RPA |
|||
Density | 0.954 g/cc | 0.0345 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® HB5502F Blow Molding HDPE High Density Polyethylene Hexene Copolymer with Synthetic Antistat Formolene® HB5502F HDPE resin is designed for applications requiring excellent stiffness and stress crack resistance properties. I.. |
|||
Density | 0.954 g/cc | 0.0345 lb/in³ | ExxonMobil method |
ExxonMobil Escorene™ UL 04331EL Ethylene Vinyl Acetate Copolymer Product Description: UL 04331EL is a HEVA grade, especially designed for photovoltaic cells and encapsulation applications, requiring a good balance of adhesion and COF. It offers excellent light tr.. |
|||
Density | 0.954 g/cc | 0.0345 lb/in³ | ExxonMobil method |
ExxonMobil Escorene™ UL 7760 Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra UL 7760 is a high viscosity, 26.7% VA copolymer that has very good flexibility and low temperature toughness. It has good compatibility with both hydrocarbon and .. |
|||
Density | 0.954 g/cc | 0.0345 lb/in³ | ISO 1183 |
ExxonMobil Exxtral™ BMU 133 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance and designed for paintable automotive exterior applications.Availability: Europe .. |
|||
Density | 0.954 g/cc | 0.0345 lb/in³ | ASTM D792, ISO 1183 |
DuPont™ Fusabond® E100 Polymer Modifier DuPont™ Fusabond® E100 is an anhydride modified high density polyethylene, mainly intended for use as a component in a blend with other polymers including polyolefins and polyamides. It is not int.. |
|||
Density | 0.954 g/cc | 0.0345 lb/in³ | ASTM D4883 |
ExxonMobil HDPE BA53-055 High Density Polyethylene Resin Product Description: BA53-055 is a high molecular weight, high density polyethylene copolymer.Availability: Latin America, North America and South America Additive: Antistatic: NoApplications: Dru.. |
|||
Density | 0.954 g/cc | 0.0345 lb/in³ | ASTM D4883 |
ExxonMobil HDPE HMA 018 High Density Polyethylene Resin Product Description: HMA 018 is an easy flow HDPE grade, characterized by high gloss and dimensional stability. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Thermal Stabili.. |
|||
Density | 0.954 g/cc | 0.0345 lb/in³ | ASTM D4883 |
ExxonMobil HDPE HYA021L High Density Polyethylene Resin Product Description: HYA021L is a molecular weight, high-density polyethylene copolymer. This resin has superior stress crack resistance, high impact strength and good rigidity.Availability: Latin A.. |
|||
Density | 0.954 g/cc | 0.0345 lb/in³ | ASTM D4883 |
ExxonMobil Paxon™ AL55-003 Blow Molding Resin Product Description: AL55-003 is a blow molding grade high density polyethylene offering a good combination of stiffness and stress crack resistance.Availability: Latin America, North America and So.. |
|||
Density | 0.954 g/cc | 0.0345 lb/in³ | ASTM D792 |
Equate EMDA-6200 HDPE Blow Molding Resin EMDA-6200 grade is a high-density polyethylene copolymer resin designed for blow molding small to medium size bottles. It can be used on intermittent as well as continuous blow molding machines for .. |
|||
Density | 0.954 g/cc | 0.0345 lb/in³ | ASTM D1505 |
Amco PRIMATOP HDPE 004955HP Blow Molding Polyethylene HDPE 003955PZ features zinc stearate additive and is used for injection blow molding.Former A-Top Polymers product; part of Amco product line since 2013. |
|||
Density | 0.954 g/cc | 0.0345 lb/in³ | ASTM D4883 |
ExxonMobil Paxon™ AM55-003 Blow Molding Resin
(discontinued **) AM55-003 is a blow molding grade high density polyethylene copolymer containing an excellent antistat additive. It provides a good combination of stiffness and stress crack resistance. AM55-003 co.. |
|||
Density | 0.954 g/cc | 0.0345 lb/in³ | ASTM D4883 |
ExxonMobil Paxon™ AU55-003 Blow Molding Resin
(discontinued **) AU55-003 is a blow molding grade high density polyethylene containing an excellent antistat additive, offering a good combination of stiffness and stress crack resistance. An enhanced additive pack.. |
|||
Density | 0.954 g/cc | 0.0345 lb/in³ | ASTM-D792 |
Braskem HB0454 HDPE Blow Molding Polyethylene Copolymer HB0454 is a high-density polyethylene copolymer resin with average molecular weight produced by the Unipol® process. A bottle made with HB0454 shows excellent processability, color, and superficial.. |