Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Exxtral™ BMU130A Performance Polyolefin

Category Polymer , Thermoplastic , Polyolefin
Manufacturer Exxon Chemical
Trade Name Exxtral™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Exxtral™ BMU130A Performance Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: Polyolefin injection molding compound with a good balance of stiffness, flow, and excellent processability for automotive bumper fascia and exterior trim applicationsAvailability: North America Features: AntistaticGood Dimensional StabilityGood FlowGood Mold ReleaseGood StiffnessLow Temperature Impact ResistancePaintable Uses: Automotive Bumper Automotive Exterior TrimProcessing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.980 g/cc
0.0354 lb/in³
ISO 1183/A
Melt Flow 15 g/10 min

@Load 2.16 kg,
Temperature 230 °C
15 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 16.0 MPa
2320 psi
ISO 527-2/50
Flexural Modulus 1.18 GPa
171 ksi
0.039 in/min; ISO 178
Izod Impact, Notched (ISO) 46.2 kJ/m²
22.0 ft-lb/in²
ISO 180/A
Multi-axial Impact @ -30°C Total Energy 7.58 J
5.59 ft-lb
14.4 ft/sec; ISO 6603-2
Thermal Properties Metric English Comments
Vicat Softening Point 118 °C
244 °F
ISO 306