Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Multi-axial Impact @ -30°C Total Energy | 7.58 J | 5.59 ft-lb | 14.4 ft/sec; ISO 6603-2 |
ExxonMobil Exxtral™ BMU130A Performance Polyolefin Product Description: Polyolefin injection molding compound with a good balance of stiffness, flow, and excellent processability for automotive bumper fascia and exterior trim applicationsAvailabilit.. |