A. Schulman POLYPUR™ FPU 1107 Thermoplastic Polyurethane Compound

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded , Polyurethane, TP
Manufacturer A. Schulman, Inc.
Trade Name POLYPUR™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYPUR™ FPU 1107 Thermoplastic Polyurethane Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
15 sec delay; ASTM D2240
Tensile Strength, Ultimate 27.0 MPa
3920 psi
at max load; ASTM D638
Elongation at Break 900 %
900 %
20 in/min; ASTM D412
Flexural Modulus 0.0260 GPa
3.77 ksi
1.3 mm/min; ASTM D790
Tear Strength 67.0 kN/m
382 pli
2 in/min; ASTM D624
Compression Set 23 %
23 %
Method B, 22 h, 23°C; ASTM D395
Thermal Properties Metric English Comments
CTE, linear 78.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
43.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM E831
Users viewing this material also viewed the following: