Mechanical Properties Metric English Comments
Multi-axial Impact @ -30°C Total Energy 7.58 J
5.59 ft-lb
14.4 ft/sec; ISO 6603-2
ExxonMobil Exxtral™ BMU130A Performance Polyolefin