Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 42.8 °C | 109 °F | ASTM D1525 |
ExxonMobil Escorene™ FL 00728CC Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00728CC is an excellent coextrusion partner in extrusion coating, blown and cast film. Good adhesion onto OPP in coextrusion. This grade offers excellent optical, low gel and.. |
|||
Vicat Softening Point | 42.8 °C | 109 °F | ASTM D1525 |
ExxonMobil Escorene™ UL 00728 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 00728 is a copolymer of ethylene and vinyl acetate.Processing Conditions: Processing temperatures above 220°C (428°F) may cause resin degradation.Availability: Africa & Mid.. |
|||
Vicat Softening Point | 42.8 °C | 109 °F | ASTM D1525 |
ExxonMobil Escorene™ UL 00728CC Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 00728CC is a copolymer of ethylene and vinyl acetate.Processing Conditions: Processing temperatures above 220°C (428°F) may cause resin degradation.Availability: Africa & M.. |
|||
Vicat Softening Point | 42.8 °C | 109 °F | ASTM D1525 |
ExxonMobil Escorene™ UL 00728FF Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 00728 is a copolymer of ethylene and vinyl acetate.Processing Conditions: Processing temperatures above 220°C (428°F) may cause resin degradation.Availability: Africa & Mid.. |
|||
Vicat Softening Point | 42.8 °C | 109 °F | at 1000g; ISO 306/A |
ExxonMobil EXACT™ 8230 Plastomer for Polymer Modification Product Description: Exact 8230 plastomer is an ethylene octene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties. It is designed.. |
|||
Vicat Softening Point | 42.8 °C | 109 °F | ASTM D1525 |
Dow AFFINITY™ EG 8100G Ethylene-octene copolymer AFFINITY™ EG 8100G Polyolefin Plastomer (POP) is produced via INSITE™ Technology. It is a general purpose ethylene-octene copolymer exhibiting high flexibility and elasticity. It can be utilized.. |
|||
Vicat Softening Point | 42.8 °C | 109 °F | ASTM D1525 |
ExxonMobil OPTEMA™ TC 220 ExCo Ethylene Methyl Acrylate Product Description: Product Description: Optema TC 220 is an ethylene methyl acrylate copolymer, which can be used for making alloys, blends and compounds or be injection molded where softness and .. |