Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Escorene® LD-760 High EVA Compounding Resin  (discontinued **)

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate; Molded/Extruded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene® LD-760 High EVA Compounding Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Exxon Chemical.A 27.5% vinyl acetate copolymer designed for specialty compounding applications. Excellent filler acceptance produces highly loaded concentrates.Applications: Compounding; Concentrates; Electrical applications.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
Exxon Method
Environmental Stress Crack Resistance >= 500 hour
>= 500 hour
F50, Condition A; ASTM D1693
Melt Flow 2.3 g/10 min
2.3 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Hardness, Shore A 76
76
ASTM D2240
Hardness, Shore D 26
26
ASTM D2240
Tensile Strength, Ultimate 17.0 MPa
2470 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Flexural Modulus 0.0260 GPa
3.77 ksi
1% Secant, ASTM D790
Tensile Impact Strength 805 kJ/m²
383 ft-lb/in²
23°C; ASTM D-1822
Thermal Properties Metric English Comments
Melting Point 73.0 °C
163 °F
Exxon Method
Vicat Softening Point 51.0 °C
124 °F
1000g; ASTM D-1525