Mechanical Properties Metric English Comments
Tensile Impact Strength 805 kJ/m²
383 ft-lb/in²
23°C; ASTM D-1822
ExxonMobil Escorene® LD-760 High EVA Compounding Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 27.5% vinyl acetate copolymer designed for specialty compounding applications. Excellent filler acceptance produces highly loaded concentrates.Ap..