Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Escorene® HD-8661 LHDPE Rotational Molding Grade  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Rotational Molding Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene® HD-8661 LHDPE Rotational Molding Grade  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Exxon Chemical.HD-8600 series are linear high density polyethylene resins that provide outstanding environmental stress crack resistance. HD-8661 is fully formulated long term UV stability package in ground form.Applications: Large agricultural tanks; Industrial products.
Physical Properties Metric English Comments
Density 0.942 g/cc
0.0340 lb/in³
Exxon Method
Environmental Stress Crack Resistance 200 hour
200 hour
F50, Condition B; ASTM D-1693
Melt Flow 2.0 g/10 min
2.0 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 18.6 MPa
2700 psi
ASTM D638
Elongation at Break 350 %
350 %
ASTM D638
Flexural Modulus 0.710 GPa
103 ksi
ASTM D790
Impact Test 237 J

@Thickness 6.35 mm,
Temperature -40.0 °C
175 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
Impact Strength; Max Force; ARM
Thermal Properties Metric English Comments
Melting Point 133 °C
271 °F
Exxon Method
Deflection Temperature at 0.46 MPa (66 psi) 54.5 °C
130 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 42.0 °C
108 °F
ASTM D648
Users viewing this material also viewed the following: