Polymer Property : Flexural Modulus = 103 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.710 GPa
103 ksi
ASTM D790
Huntsman Rexell® H2110 Injection Molding LLDPE  (discontinued **)
Linear-low high density injection molding.Features: Good toughness, ESCR.Applications: Industrial and consumer pails, general purpose molding.Information provided by Huntsman Corporation
Flexural Modulus 0.710 GPa
103 ksi
ASTM D790
ExxonMobil Escorene® HD-8660 HDPE, Rotational Molding Pellets  (discontinued **)
Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated UV-8 type protection, Higher stiffness & impact strengthUses: Large agricultural tanks, Industrial products
Flexural Modulus 0.710 GPa
103 ksi
ASTM D790
ExxonMobil Escorene® HD-8661 HDPE, Rotational Molding Powder  (discontinued **)
Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated UV-8 type protection, Higher stiffness & impact strengthUses: Large agricultural tanks, Industrial products
Flexural Modulus 0.710 GPa
103 ksi
ASTM D790
ExxonMobil Escorene® HD-8660 LHDPE Rotational Molding Grade  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.HD-8600 series are linear high density polyethylene resins that provide outstanding environmental stress crack resistance. HD-8660 is fully formula..
Flexural Modulus 0.710 GPa
103 ksi
ASTM D790
ExxonMobil Escorene® HD-8661 LHDPE Rotational Molding Grade  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.HD-8600 series are linear high density polyethylene resins that provide outstanding environmental stress crack resistance. HD-8661 is fully formula..
Flexural Modulus 0.710 GPa
103 ksi
80x10x4 mm specimen, 2 mm/min; ISO 178
Solvay Engineered Polymers DEXFLEX® 826HS TPO  (discontinued **)
Description: DEXFLEX® 826HS is a thermoplastic olefinic elastomer (TPO) designed for automotive exterior applications that require a combination of stiffness, low-temperature impact resistance, and..