Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eurostar Starpylen HZ 30WF2 PP, 30% Wood Fiber Filled, Injection Molding

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Wood Filled
Manufacturer Eurostar Engineering Plastics
Trade Name Starpylen
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurostar Starpylen HZ 30WF2 PP, 30% Wood Fiber Filled, Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Starpylen HZ 30WF2 is a 30% Wood Fiber Reinforced Polypropylene Injection Molding Resin (also known as HZ30WF2)Information provided by Eurostar.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
ISO 1183
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 29.0 MPa
4210 psi
ISO 527
Elongation at Break 3.5 %
3.5 %
ISO 527
Tensile Modulus 2.30 GPa
334 ksi
1 mm/min; ISO 527
Flexural Modulus 2.68 GPa
389 ksi
ISO 178
Charpy Impact Unnotched 1.70 J/cm²
8.09 ft-lb/in²
Edgew 80x10x4 sp=62; ISO 179/1eU
Processing Properties Metric English Comments
Zone 1 185 - 195 °C
365 - 383 °F
Zone 2 185 - 195 °C
365 - 383 °F
Zone 3 185 - 195 °C
365 - 383 °F
Melt Temperature 185 - 195 °C
365 - 383 °F
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Drying Temperature 70.0 °C

@Time 10800 sec
158 °F

@Time 3.00 hour