Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 77
77
15 sec; ASTM D2240
Tensile Strength at Break 17.1 MPa
2480 psi
Type IV, 510 mm/min; ASTM D638
Tensile Strength 10.3 MPa

@Strain 100 %
1490 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
Elongation at Break 320 %
320 %
Type IV, 510 mm/min; ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -32.8 °C
-27.0 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 177 - 182 °C
351 - 360 °F
188 - 199 °C
370 - 390 °F
Descriptive Properties Value Comments
Appearance Clear/Transparent
Features High Clarity
High Gloss
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Furniture
Hose
Tubing