Polymer Property : Flexural Modulus, 1% Secant = 139000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 960 MPa
139000 psi
ASTM D 790
NOVA Chemicals Sclair® IG454-A Injection Molded HDPE Resin
IG454-A complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. IG454..
Flexural Modulus, 1% Secant 960 MPa
139000 psi
ASTM D790
Entec Hypro™ PP-CP35/1.5C Impact Copolymer, 35 Melt Flow
This product is intended for general purpose injection molding applications especially those requiring fast cycle time, improved color, enhanced processability, and excellent clarity.Information pro..
Flexural Modulus, 1% Secant 960 MPa
139000 psi
ASTM-D790
Braskem GV0350 HDPE Blow Molding Polyethylene Copolymer
HDPE GV0350 is a high-density polyethylene copolymer that has great molar mass, excellent chemical resistance, and high impact resistance and stiffness. It was developed for the blow-molding of larg..