Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ensinger Hydel® PC-7 Polycarbonate (PC)

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Carbon Fiber Reinforced
Manufacturer Ensinger
Trade Name Hydel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Hydel® PC-7 Polycarbonate (PC).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A polycarbonate based material with a proprietary carbon filler component. The highly dispersed filler imparts outstanding electrical consistency to minimize any hot spots. The material has good repeatability and predictability of any commercially available carbon based filler. HYDEL® PC-7 has minimal sloughing as compared to other carbon based fillers. This material also retains much of the physical properties of polycarbonate without the loss of impact and tensile properties that can occur with standard carbon based or fiber fillers.Information Provided by Ensinger Industries, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Water Absorption 0.15 %

@Temperature 22.8 °C,
Time 86400 sec
0.15 %

@Temperature 73.0 °F,
Time 24.0 hour
ASTM D570
Water Absorption at Saturation 0.15 %
0.15 %
Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.1 MPa
9000 psi
ASTM D638
Elongation at Break 8.0 %
8.0 %
ASTM D638
Tensile Modulus 2.30 GPa
333 ksi
ASTM D638
Flexural Strength 74.5 MPa
10800 psi
ASTM D790
Flexural Modulus 2.34 GPa
340 ksi
ASTM D790
Compressive Strength 84.8 MPa
12300 psi
ASTM D695
Izod Impact, Notched 0.641 J/cm
1.20 ft-lb/in
ASTM D256
Coefficient of Friction, Dynamic 0.12

@Pressure 0.276 MPa
0.12

@Pressure 40.0 psi
50 fpm
Thermal Properties Metric English Comments
CTE, linear 66.6 µm/m-°C
37.0 µin/in-°F
Maximum Service Temperature, Air 127 °C
260 °F
continuous
Deflection Temperature at 1.8 MPa (264 psi) 138 °C
280 °F
ASTM D648
Flammability, UL94 V-2
V-2
Electrical Properties Metric English Comments
Surface Resistivity per Square 1e+05 - 1.00e+7 ohm
1e+05 - 1.00e+7 ohm
ASTM D257
Descriptive Properties Value Comments
Base Material Polycarbonate