Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 66.6 µm/m-°C @Temperature 20.0 °C |
37.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Lubrizol ISOPLAST™ 202EZ Engineering Thermoplastic Polyurethane Resin NSF Standard 61 CertifiedAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
CTE, linear | 66.6 µm/m-°C @Temperature 20.0 °C |
37.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
CPC - Vycom FLAMETEC™ CPVC Chlorinated Polyvinyl Chloride Sheet Flametec™ CPVC made from Corzan® 4910 white 120 compound is a high heat, corrosion resistant chlorinated polyvinyl chloride sheet. Because of its excellent corrosion resistance at elevated tempera.. |
|||
CTE, linear | 66.6 µm/m-°C | 37.0 µin/in-°F | |
Ensinger Hydel® PC-7 Polycarbonate (PC) A polycarbonate based material with a proprietary carbon filler component. The highly dispersed filler imparts outstanding electrical consistency to minimize any hot spots. The material has good r.. |
|||
CTE, linear | 66.6 µm/m-°C | 37.0 µin/in-°F | ASTM D696 |
Ensinger Hydex™ 202 Rigid Polyurethane (PU) Hydex™ 202 is a totally rigid polyurethane resin that exhibits a broad range of chemical resistance, as well as superior impact and excellent mechanical properties. It can be used for any mechanic.. |
|||
CTE, linear | 66.6 µm/m-°C @Temperature 20.0 °C |
37.0 µin/in-°F @Temperature 68.0 °F |
|
Aremco Aremco-Bond™ 2300 High Performance Epoxide Milky Clear, 10:1, Low Viscosity, Exceptional Bond Strength. |
|||
CTE, linear | 66.6 µm/m-°C @Temperature 20.0 °C |
37.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Axiall 7048A Rigid PVC, Extrusion Georgia Gulf 7048A is a general purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Impact Strength & ToughnessFlame RetardantColorabilityCert.. |
|||
CTE, linear | 66.6 µm/m-°C | 37.0 µin/in-°F | |
BCC Products BC 7062-2H Epoxy Casting BC 7062 are aluminum filled, low viscosity epoxy mass casting resins. These room temperature cure systems allow the user choice thicknesses of 1/8 inch to a maximum of 6 inches without foaming or yi.. |