Elastomer Engineering E50D Polyurethane

Category Polymer , Thermoplastic , Polyester, TP , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Elastomer Engineering
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Elastomer Engineering E50D Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A polyester-based urethane with excellent strength, resilience, and abrasion resistance. Excellent in heavy-duty applications and where oils and solvents are present. Information provided by Elastomer Engineering Inc (EEI)
Mechanical Properties Metric English Comments
Hardness, Shore D 51
51
Tensile Strength, Ultimate 48.3 MPa
7000 psi
Elongation at Break 500 %
500 %
100% Modulus 0.0105 GPa
1.53 ksi
300% Modulus 0.0207 GPa
3.00 ksi
Rebound 33 %
33 %
Bayshore
Tear Strength 64.0 kN/m
365 pli
Split
109 kN/m
620 pli
Die C
Compression Set 36 %
36 %
Method B