300% Modulus 0.0207 GPa
3.00 ksi
Dow Pellethane® 2102-90AE Polyurethane Elastomer, Polyester Polycaprolactone Based  (discontinued **)
PELLETHANE® 2102-90AE elastomer is a polyester polycaprolactone based polyurethane elastomer which combines excellent resistance to fuels and oils with good damping capacity and good hydrolytic sta..
300% Modulus 0.0207 GPa
3.00 ksi
ASTM D412
Lubrizol Pellethane® 2363-90A Thermoplastic Polyurethane Elastomer
Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
300% Modulus 0.0207 GPa
3.00 ksi
Elastomer Engineering E50D Polyurethane
A polyester-based urethane with excellent strength, resilience, and abrasion resistance. Excellent in heavy-duty applications and where oils and solvents are present. Information provided by Elasto..
300% Modulus 0.0207 GPa
3.00 ksi
ASTM D412
Lubrizol ESTANE® 58226 Ester Based Thermoplastic Polyurethane
Features: Excellent physical properties, good chemical resistance and enhanced hydrolysis resistance. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and..