Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0105 GPa | 1.53 ksi | |
Elastomer Engineering E50D Polyurethane A polyester-based urethane with excellent strength, resilience, and abrasion resistance. Excellent in heavy-duty applications and where oils and solvents are present. Information provided by Elasto.. |