A. Schulman POLYAXIS® LPA815 LPA 815EVA

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate; Molded/Extruded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYAXIS® LPA815 LPA 815EVA.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolyaxis LPA 815 is an EVA which is soft an pliable, even at low temperatures.NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and ESCR tests were performed on compression molded samples. ApplicationApplications of Polyaxis® LPA 815 include toys, dock bumpers and floats. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.935 g/cc
0.935 g/cc
ASTM D792
Vinyl Acetate Content 15 %
15 %
by weight
Melt Index of Compound 6.0 - 8.0 g/10 min
6.0 - 8.0 g/10 min
2.16/190; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 14.5 MPa
2100 psi
2"/min; ASTM D638
Elongation at Break 700 %
700 %
2"/min; ASTM D638
Flexural Modulus 0.0593 GPa
8.60 ksi
at 1% secant modulus; ASTM D790