Material Notes:
Voridian polyethylene E6838-010A is a low density formulation with medium slip used for injection molding. It is an outstanding material for molding lids and other container closures because it processes easily on automated molding equipment to produce molded items with excellent gloss, clarity, and warpage resistance. Users must make their own determination that use of this product is safe, legal, and technically suitable for their intended applications.Information from manufacturer data sheet.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D 4883
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 8.00 MPa
1160 psi
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Tensile Strength, Yield 11.0 MPa
1600 psi
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Elongation at Break 90 %
90 %
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Flexural Modulus 0.228 GPa
33.1 ksi
2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 90.0 °C
194 °F
ASTM D1525
Brittleness Temperature -45.0 °C
-49.0 °F
ASTM D746
Descriptive Properties Value Comments
Process Injection