Material Notes:
Voridian polyethylene D4009-A is a low density formulation used for injection molding. It is an outstanding material for molding lids and other container closures because it processes easily on automatic molding equipment to produce molded items with excellent gloss, clarity, and warpage resistance.Information supplied by the manufacturer.Information from manufacturer data sheet.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D4883
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 8.00 MPa
1160 psi
500 mm/min (20 in./min.); Type IV Specimen; ASTM D638
Tensile Strength, Yield 11.0 MPa
1600 psi
500 mm/min (20 in./min.); Type IV Specimen; ASTM D638
Elongation at Break 90 %
90 %
500 mm/min (20 in./min.); Type IV Specimen; ASTM D638
Flexural Modulus 0.228 GPa
33.1 ksi
2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 90.0 °C
194 °F
ASTM D1525
Brittleness Temperature -45.0 °C
-49.0 °F
ASTM D746
Descriptive Properties Value Comments
Process Injection