Eastman Tritan FX100 Copolyester

Category Polymer , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer Eastman Chemical
Trade Name Tritan
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman Tritan FX100 Copolyester.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Eastman Tritan FX100 is an amorphous copolyester that combines clarity and toughness with heat and chemical resistance. Films manufactured from this new-generation copolyester can be thermoformed without pre-drying and with a wide processing window that allows for product designs that reflect intricate detail.Application/UsesConsumer and durable goodsGraphic artsLeisure and safetySpecialty filmsKey AttributesDoes not contain Bisphenol-A (BPA)Does not contain plasticizersExcellent clarityGood heat resistanceNo pre-drying of film prior to thermoformingOutstanding chemical resistanceGood toughnessWide thermoforming windowInformation was provided by Eastman.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D1505
Water Absorption 0.50 %

@Time 86400 sec
0.50 %

@Time 24.0 hour
ASTM D570
Water Vapor Transmission 4.00 g/m²/day

@Temperature 23.0 °C
0.258 g/100 in²/day

@Temperature 73.4 °F
ASTM F1249
11.0 g/m²/day

@Temperature 38.0 °C
0.708 g/100 in²/day

@Temperature 100 °F
ASTM F1249
Oxygen Transmission 32.0 cc-mm/m²-24hr-atm
81.3 cc-mil/100 in²-24hr-atm
ASTM D3985
Carbon Dioxide Transmission 149 cc-mm/m²-24hr-atm
378 cc-mil/100 in²-24hr-atm
ASTM D1434
Thickness 254 microns
10.0 mil
Thickness of film tested; ASTM D374
Surface Tension 8.0 dynes/cm
8.0 dynes/cm
Polar; ASTM D5946
39 dynes/cm
39 dynes/cm
Dispersive; ASTM D5946
46 dynes/cm
46 dynes/cm
Total; ASTM D5946
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 41.0 MPa
5950 psi
ASTM D882
Film Tensile Strength at Yield, TD 40.0 MPa
5800 psi
ASTM D882
Film Elongation at Break, MD 179 %
179 %
ASTM D882
Film Elongation at Break, TD 203 %
203 %
ASTM D882
Film Elongation at Yield, MD 7.0 %
7.0 %
ASTM D882
Film Elongation at Yield, TD 7.0 %
7.0 %
ASTM D882
Secant Modulus, MD 1.50 GPa
218 ksi
Tangent; ASTM D882
Secant Modulus, TD 1.40 GPa
203 ksi
Tangent; ASTM D882
Puncture Energy 4.60 J
3.39 ft-lb
Dynatup; ASTM D3763
Tear Strength 11.0 kN/m
62.8 pli
MD; Trouser @200/mm/min; ISO 6383-1
11.0 kN/m
62.8 pli
TD; Trouser @200/mm/min; ISO 6383-1
12.0 kN/m
68.5 pli
Split tear method, TD; ASTM D1938
13.0 kN/m
74.2 pli
Split tear method, MD; ASTM D1938
Elmendorf Tear Strength MD 520 g
520 g
ASTM D1922
Elmendorf Tear Strength TD 571 g
571 g
ASTM D1922
Elmendorf Tear Strength, MD 2.00 g/micron
50.8 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 2.20 g/micron
55.9 g/mil
ASTM D1922
Dart Drop 3.50 g/micron

@Temperature 23.0 °C
88.9 g/mil

@Temperature 73.4 °F
ASTM 1709A
3.60 g/micron

@Temperature -30.0 °C
91.4 g/mil

@Temperature -22.0 °F
ASTM 1709A
Dart Drop Test 882 g

@Temperature 23.0 °C
1.94 lb

@Temperature 73.4 °F
ASTM 1709A
913 g

@Temperature -30.0 °C
2.01 lb

@Temperature -22.0 °F
ASTM 1709A
Film Tensile Strength at Break, MD 59.0 MPa
8560 psi
ASTM D882
Film Tensile Strength at Break, TD 52.0 MPa
7540 psi
ASTM D882
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
ASTM D696
Specific Heat Capacity 1.72 J/g-°C

@Temperature 60.0 °C
0.410 BTU/lb-°F

@Temperature 140 °F
DSC
1.88 J/g-°C

@Temperature 100 °C
0.450 BTU/lb-°F

@Temperature 212 °F
DSC
2.26 J/g-°C

@Temperature 150 °C
0.540 BTU/lb-°F

@Temperature 302 °F
DSC
2.43 J/g-°C

@Temperature 200 °C
0.580 BTU/lb-°F

@Temperature 392 °F
DSC
2.59 J/g-°C

@Temperature 250 °C
0.620 BTU/lb-°F

@Temperature 482 °F
DSC
Glass Transition Temp, Tg 110 °C
230 °F
DSC
Optical Properties Metric English Comments
Refractive Index 1.55
1.55
ASTM D542
Haze 0.70 %
0.70 %
ASTM D1003
Gloss 161 %
161 %
@ 60°; ASTM D2457
Yellow Index 0.50 %
0.50 %
ASTM D1925
Transmission, Visible 92 %
92 %
ASTM D1003
UV Transmittance 89 %

@Thickness 0.380 mm
89 %

@Thickness 0.0150 in
UV/Vis Spectro
Compliance Properties Metric English Comments
FDA Yes
Yes
Repeated use food contact articles
NSF Yes
Yes
Food equipment materials; NSF/ANSI Standard 51
Descriptive Properties Value Comments
PPT Tear Resistance, M.D. 42 N
ASTM D2582
PPT Tear Resistance, T.D. 56 N
ASTM D2582
Taber Abrasion 23% haze
ASTM 1044, Average at 25 cycles