Mechanical Properties Metric English Comments
Tear Strength 12.0 kN/m
68.5 pli
ASTM D624B
P & P Technology CB 70 Carbon Loaded Silicone
Applications: Electrically conductive grades which when properly catalyzed can be considered for applications requiring conductivity such as EMI gaskets, conductive sheaths for ignition cable core,..
Tear Strength 12.0 kN/m
68.5 pli
12 kN/m at 23°C. Value at 100°C is 3.6 kN/m. TPE-0056 (ASTM D 624)
ExxonMobil Santoprene® 8211-35W237 Thermoplastic Rubber  (discontinued **)
A colorable thermoplastic general purpose non-hygroscopic elastomer, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can be processe..
Tear Strength 12.0 - 16.0 kN/m
68.5 - 91.3 pli
NF EN ISO 1421
Isoflon Tisoflon® 3G Polytetrafluoroethylene & Graphite Coated Glass Fabric
PTFE + Graphite coated glass fabric TISOFLON® - Black anti-staticInformation provided by Isoflon.
Tear Strength >= 12.0 kN/m
>= 68.5 pli
DIN 53507
Karina 300-40/236 Green PVC Compound
For footware.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tear Strength >= 12.0 kN/m
>= 68.5 pli
DIN 53507
Karina 35/200 Clear PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tear Strength 12.0 kN/m
68.5 pli
Die B
Momentive Performance Materials Siloprenâ„¢ LSR 3696/20 Liquid Silicone Rubber - Self-Lubricating / Ultra Low Compression Set
This LSR elastomer is a self-lubricating, ultra low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycl..
Tear Strength 12.0 kN/m
68.5 pli
Trelleborg R608 Commercial Natural Rubber Polyisoprene
All information provided by Trelleborg
Tear Strength 12.0 kN/m
68.5 pli
Trelleborg R661 Natural Rubber Polyisoprene
All information provided by Trelleborg
Tear Strength 12.0 kN/m
68.5 pli
Split tear method, TD; ASTM D1938
Eastman Tritan FX100 Copolyester
Eastman Tritan FX100 is an amorphous copolyester that combines clarity and toughness with heat and chemical resistance. Films manufactured from this new-generation copolyester can be thermoformed w..
Tear Strength 12.0 kN/m
68.5 pli
Split tear method, TD; ASTM D1938
Eastman Tritan MP100 Copolyester
Eastman Tritan MP100 is an amorphous copolyester that combines excellent clarity and toughness with outstanding heat and chemical resistance. Film and sheet manufactured from this new-generation co..
Tear Strength 12.0 kN/m
68.5 pli
73°C, Die C; ASTM D624
ExxonMobil Santoprene® 8281-45MED Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of..
Tear Strength 12.0 kN/m
68.5 pli
Trelleborg R660 Natural Rubber Polyisoprene
All information provided by Trelleborg
Tear Strength 12.0 kN/m
68.5 pli
Trelleborg Z600 Commercial SBR Rubber
Styrene-butadiene Rubber is a co-polymer of styrene and butadiene.PropertiesIts general properties are similar to those of natural rubber, but it is more resistant to aging and temperature, and like..
Tear Strength 12.0 kN/m
68.5 pli
ISO 34-B
AlphaGary Evoprene™ G 3290 SEBS Thermoplastic Elastomer
Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi..
Tear Strength 12.0 kN/m
68.5 pli
ISO 34-B
AlphaGary Evoprene™ GC 5677 SEBS Thermoplastic Elastomer
Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can..