Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 11.0 - 114 kN/m | 62.8 - 650 pli | Average value: 56.1 kN/m Grade Count:72 |
Overview of materials for PVC, Flexible Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Flexible Grade". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Tear Strength | 11.0 kN/m | 62.8 pli | 70°C for 1,000 hrs; JIS-K-6252 |
Fujipoly Industries Sarcon® 25G-Td Thin-Film GR-TD Sarcon 25G-Td is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary.Information provided by Fujipoly Industries |
|||
Tear Strength | 11.0 kN/m | 62.8 pli | Die C; ASTM D624 |
Teknor Apex Uniprene® 35A Polyvinyl Chloride, Flexible Features: High Elastic RecoveryInformation Provided by Teknor Apex |
|||
Tear Strength | 11.0 kN/m | 62.8 pli | MD; Trouser @200/mm/min; ISO 6383-1 |
Eastman Tritan FX100 Copolyester Eastman Tritan FX100 is an amorphous copolyester that combines clarity and toughness with heat and chemical resistance. Films manufactured from this new-generation copolyester can be thermoformed w.. |
|||
Tear Strength | 11.0 kN/m | 62.8 pli | TD; Trouser @200/mm/min; ISO 6383-1 |
Eastman Tritan FX100 Copolyester Eastman Tritan FX100 is an amorphous copolyester that combines clarity and toughness with heat and chemical resistance. Films manufactured from this new-generation copolyester can be thermoformed w.. |
|||
Tear Strength | 11.0 kN/m | 62.8 pli | MD; Trouser @200/mm/min; ISO 6383-1 |
Eastman Tritan MP100 Copolyester Eastman Tritan MP100 is an amorphous copolyester that combines excellent clarity and toughness with outstanding heat and chemical resistance. Film and sheet manufactured from this new-generation co.. |
|||
Tear Strength | 11.0 kN/m | 62.8 pli | TD; Trouser @200/mm/min; ISO 6383-1 |
Eastman Tritan MP100 Copolyester Eastman Tritan MP100 is an amorphous copolyester that combines excellent clarity and toughness with outstanding heat and chemical resistance. Film and sheet manufactured from this new-generation co.. |
|||
Tear Strength | 11.0 kN/m | 62.8 pli | |
Trelleborg Commercial Neoprene® C400 Chloroprene CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade.. |
|||
Tear Strength | 11.0 kN/m | 62.8 pli | ISO 34-B |
AlphaGary Evoprene™ GC 5685 SEBS Thermoplastic Elastomer Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can.. |