Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 12.0 kN/m | 68.5 pli | ASTM D624B |
P & P Technology CB 70 Carbon Loaded Silicone Applications: Electrically conductive grades which when properly catalyzed can be considered for applications requiring conductivity such as EMI gaskets, conductive sheaths for ignition cable core,.. |
|||
Tear Strength | 12.0 - 71.0 kN/m | 68.5 - 405 pli | Average value: 33.9 kN/m Grade Count:5 |
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum.. |
|||
Tear Strength | >= 12.0 kN/m | >= 68.5 pli | DIN 53507 |
Karina 300-40/236 Green PVC Compound For footware.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tear Strength | 12.0 kN/m | 68.5 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ Electro 940 Liquid Silicone Rubber - Medium Voltage This LSR elastomer is a medium voltage, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperat.. |
|||
Tear Strength | 12.0 kN/m | 68.5 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 3696/20 Liquid Silicone Rubber - Self-Lubricating / Ultra Low Compression Set This LSR elastomer is a self-lubricating, ultra low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycl.. |
|||
Tear Strength | 12.0 - 16.0 kN/m | 68.5 - 91.3 pli | NF EN ISO 1421 |
Isoflon Tisoflon® 3 AD Polytetrafluoroethylene Coated Glass Fabric PTFE coated glass fabric one side adhesive TISOFLON® - Standard gradeInformation provided by Isoflon. |
|||
Tear Strength | 12.0 kN/m | 68.5 pli | |
Trelleborg R661 Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tear Strength | 12.0 kN/m | 68.5 pli | Split tear method, TD; ASTM D1938 |
Eastman Tritan FX100 Copolyester Eastman Tritan FX100 is an amorphous copolyester that combines clarity and toughness with heat and chemical resistance. Films manufactured from this new-generation copolyester can be thermoformed w.. |
|||
Tear Strength | 12.0 kN/m | 68.5 pli | Split tear method, TD; ASTM D1938 |
Eastman Tritan MP100 Copolyester Eastman Tritan MP100 is an amorphous copolyester that combines excellent clarity and toughness with outstanding heat and chemical resistance. Film and sheet manufactured from this new-generation co.. |
|||
Tear Strength | 12.0 kN/m | 68.5 pli | 73°C, Die C; ASTM D624 |
ExxonMobil Santoprene® 8281-45MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Tear Strength | 12.0 kN/m | 68.5 pli | |
Trelleborg Z600 Commercial SBR Rubber Styrene-butadiene Rubber is a co-polymer of styrene and butadiene.PropertiesIts general properties are similar to those of natural rubber, but it is more resistant to aging and temperature, and like.. |
|||
Tear Strength | 12.0 kN/m | 68.5 pli | ISO 34-B |
AlphaGary Evoprene™ GC 5677 SEBS Thermoplastic Elastomer Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can.. |