Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eastman D4056-P Polyethylene  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman D4056-P Polyethylene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polyethylene D4056-P is a natural low density material with an 80 melt index.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line.
Physical Properties Metric English Comments
Density 0.911 g/cc
0.0329 lb/in³
ASTM D4883
Melt Flow 80 g/10 min

@Load 2.16 kg,
Temperature 190 °C
80 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 6.90 MPa
1000 psi
500 mm/min; ASTM D638
Tensile Strength, Yield 8.30 MPa
1200 psi
500 mm/min; ASTM D638
Elongation at Break 120 %
120 %
500 mm/min; ASTM D638
Flexural Modulus 0.138 GPa
20.0 ksi
2% Secant, 12.7 mm/min; ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 71.0 °C
160 °F
ASTM D1525
Descriptive Properties Value Comments
Process Film
Users viewing this material also viewed the following: