Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength at Break = 1000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 6.90 MPa
1000 psi
NuSil R1-2145 Silicone Two Part Sealing & Adhesive
General Purpose: Two Part Sealing & AdhesiveComments: Longer Work Time, Young's Modulus 300 psi (2.1 MPa)Cure System: PlatinumInformation provided by NuSil
Tensile Strength at Break 6.90 MPa
1000 psi
NuSil R-2615-3 Silicone Two Part Sealing & Adhesive
General Purpose: Two Part Sealing & AdhesiveComments: Low ViscosityCure System: PlatinumInformation provided by NuSil
Tensile Strength at Break 6.90 MPa
1000 psi
NuSil R31-2186 Silicone Two Part Sealing & Adhesive
General Purpose: Two Part Sealing & AdhesiveComments: Flowable, Fast Cure AdhesiveCure System: PlatinumInformation provided by NuSil
Tensile Strength at Break 6.90 MPa
1000 psi
NuSil CV10-2500 Silicone, Two Part Adhesive and Sealant
General Purpose: Two Part Adhesive and SealantComments: High Durometer, Optically ClearCure system: PlatinumInformation provided by NuSil
Tensile Strength at Break 6.90 MPa
1000 psi
NuSil CV-2500 Silicone, Two Part Adhesive and Sealant
General Purpose: Two Part Adhesive and SealantComments: Pourable, Optically ClearCure system: PlatinumInformation provided by NuSil
Tensile Strength at Break 6.90 MPa
1000 psi
Certified
NuSil MED-4770 Ultra High Performance High Consistency Elastomers - Unrestricted Medical Use
Description: High consistency rubber, or HCR, consists of high molecular weight polymer combined with silica to produce a material that can be molded, extruded, or calendared into a useful end produ..
Tensile Strength at Break 6.89 MPa
1000 psi
Across flow; ASTM D412
ExxonMobil Santoprene® 8291-65TB Thermoplastic Rubber  (discontinued **)
Description: A colorable thermoplastic elastomer which bonds to adhesive/epoxy spin-finished polyester or standard nylon fibers for closed-braid hose and woven-substrate products. With bonds strong..
Tensile Strength at Break 6.90 MPa
1000 psi
500 mm/min; ASTM D638
Eastman D4056-P Polyethylene  (discontinued **)
Polyethylene D4056-P is a natural low density material with an 80 melt index.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no lon..
Tensile Strength at Break 6.90 MPa
1000 psi
Typical
NuSil MED2-4013 Silicone, One Part Adhesive/Sealant - Restricted Medical Use
Description: Silicone adhesives are elastomers or pressure sensitive adhesive systems that are designed to bond silicone surfaces to each other and to other substrate surfaces such as metals and pla..
Tensile Strength at Break 6.91 MPa
1000 psi
ISO R 527
Stir SpA B 3060 AT (PVC)
Application: Molding for boot-legInformation provided by STIR SpA
Tensile Strength at Break 6.89 MPa
1000 psi
ASTM D412
Teknor Apex Monprene® MP-1518C Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 6.89 MPa
1000 psi
ASTM D412
Teknor Apex Monprene® MP-1650L2 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 6.89 MPa
1000 psi
ASTM D412
Teknor Apex Monprene® MP-1766B Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 6.89 MPa
1000 psi
ASTM D412
Teknor Apex Monprene® MP-2132 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 6.89 MPa
1000 psi
ASTM D412
Teknor Apex Monprene® MP 1257 Thermoplastic Elastomer
Notes: General Purpose; CSA Approved; OpaqueInformation Provided by Teknor Apex
Tensile Strength at Break 6.89 MPa
1000 psi
ASTM D412
Teknor Apex Monprene® MP-2776A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 6.89 MPa
1000 psi
ASTM D412
Teknor Apex Monprene® MP-2815C Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 6.89 MPa
1000 psi
ASTM D412
Teknor Apex Monprene® MP-2870M Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 6.89 MPa
1000 psi
ASTM D412
Teknor Apex Telcar® OBC 4864A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Tensile Strength at Break 6.89 MPa
1000 psi
ASTM D412
Teknor Apex Telcar® TL-1295B Thermoplastic Elastomer
Uses: Consumer Applications; General Purpose; Soft Touch Applications; Flexible Grips; Handles; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: M..
Tensile Strength at Break 6.89 MPa
1000 psi
ASTM D412
Teknor Apex Telcar® TL-2433A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Tensile Strength at Break 6.89 MPa
1000 psi
ASTM D412
Teknor Apex Telcar® TL-2540F Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Tensile Strength at Break 6.89 MPa
1000 psi
ASTM D412
Teknor Apex Telcar® TL-91-T3056D-75 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Tensile Strength at Break 6.89 MPa
1000 psi
ASTM D638
Teknor Apex Vidux® CV-98-PO323-G79 Polyvinyl Chloride, Flexible
Notes: 105°C Insulation Features: Conductive; Good Abrasion Resistance; Flame Retardant; Good Wear Resistance Uses: Tubing Forms: BlackInformation Provided by Teknor Apex
Tensile Strength at Break 6.89 MPa

@Thickness 3.20 mm
1000 psi

@Thickness 0.126 in
Die C; 20 in/min (500 mm/min); ASTM D 412
RTP Company RTP 2800 B-85A FR A Thermoplastic Polyolefin Elastomer (TEO) Flame Retardant - PBDE Free
Tensile Strength at Break 6.89 MPa
1000 psi
ASTM D638
ExxonMobil HDPE HD 6605.70 High Density Polyethylene Copolymer Resin
Product Description: HD 6605.70 is a narrow molecular weight hexane copolymer designed for a wide range of injection molding applications, offering excellent ESCR with good stiffness-toughness balan..
Tensile Strength at Break 6.89 MPa

@Thickness 3.17 mm
1000 psi

@Thickness 0.125 in
Die C; 20 in/min (500 mm/min); ASTM D412
RTP Company RTP 2800 B-75A Thermoplastic Polyolefin Elastomer (TEO)  (discontinued **)
Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Tensile Strength at Break 6.90 MPa
1000 psi
Across Flow; ASTM D412 and ISO 37
ExxonMobil Santoprene® 201-67W171 Thermoplastic Vulcanizate  (discontinued **)
Product Description: A soft, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is specially formulated for low density foamed profile extrusion ap..
Tensile Strength at Break 6.89 MPa

@Thickness 3.20 mm
1000 psi

@Thickness 0.126 in
Die C; 20 in/min (500 mm/min); ASTM D 412
RTP Company RTP 6042-50A UV BLACK Specialty Thermoplastic Elastomer, UV Stabilized - Bondable to ABS, PC, PC Alloys, PBT, RTPU
Tensile Strength at Break 6.89 MPa
1000 psi
ASTM D412
Compuestos Dominicanos Polycom CH-550140 PVC Compound
Compuestos Dominicanos SA produces a wide variety of PVC compounds for the injection molding of footwear products; everything from full injection, shoe soles, boots, and PVC compounds for oil resist..