Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 80 g/10 min @Load 2.16 kg, Temperature 210 °C |
80 g/10 min @Load 4.76 lb, Temperature 410 °F |
ASTM D1238 |
NatureWorks® Ingeo™ 6252D Meltblown Fiber Grade Biopolymer NatureWorks® PLA polymer 6252D is a thermoplastic fiber-grade resin derived from annually renewable resources. Available in lubricated pellet form, 6252D is designed for meltblown products using co.. |
|||
Melt Flow | 80 g/10 min @Load 2.16 kg, Temperature 190 °C |
80 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Eastman D4056-P Polyethylene
(discontinued **) Polyethylene D4056-P is a natural low density material with an 80 melt index.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no lon.. |
|||
Melt Flow | 80 - 120 g/10 min | 80 - 120 g/10 min | Melt Volume Rate (cm³/10 min) |
Huntsman IROGRAN® A 78 P 4766 TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
Melt Flow | 80 g/10 min @Load 2.16 kg, Temperature 230 °C |
80 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Ineos L80Z-00 Impact Copolymer Polypropylene L80Z-000 impact copolymer polypropylene is a high melt flow rate, nucleated and antistatic grade designed for high-speed injection molding applications. This resin meets the requirements of the U.S... |
|||
Melt Flow | 80 g/10 min @Load 2.16 kg, Temperature 250 °C |
80 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® HX215HP PBT High Flow, Unreinforced, Polybutylene Terephthalate (PBT). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food conta.. |
|||
Melt Flow | 80 g/10 min @Load 1.20 kg, Temperature 300 °C |
80 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Styron CALIBREâ„¢ 1080 DVD Polycarbonate CALIBREâ„¢ 1080 DVD resin has been developed to meet the high demands of the modern Optical Media Industry and is suitable for standard CD molding (audio or ROM) as well as for recordable optical.. |
|||
Melt Flow | 80 g/10 min @Load 2.16 kg, Temperature 230 °C |
80 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis BJ380MO Polypropylene Copolymer BJ380MO is a very high melt flow heterophasic copolymer with high/medium impact strength and stiffness. This grade is designed for high-speed injection molding and contains nucleating and antistatic.. |
|||
Melt Flow | 80 g/10 min @Load 2.16 kg, Temperature 190 °C |
80 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Westlake EC4056AA Low Density Polyethylene WESTLAKE low-density polyethylene EC4056 is a natural low density material with an 80 melt index.FDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.All in.. |
|||
Melt Flow | 80 g/10 min @Load 2.16 kg, Temperature 230 °C |
80 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Total PPR 12232 Random Copolymer Polypropylene Total Petrochemicals PPR 12232 is a high melt flow index, high transparency random copolymer. Its has an excellent food compatibility due to its low odor, making it especially suitable for the produ.. |
|||
Melt Flow | 80 g/10 min | 80 g/10 min | ASTM D1238 |
Total PPC 5945WZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 5945WZ is a nucleated impact copolymer with a Melt Flow index of 80 g/10 min.TOTAL Polypropylene 5945WZ is characterized by very low warpage, improved stiffness, a.. |
|||
Melt Flow | 80 g/10 min @Load 5.00 kg, Temperature 230 °C |
80 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
ELASTO UK Dryflex® 3031-102 TPE, Modified Injection Molding Grade for Auto Interior Parts The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 3031-102 is specifically designe.. |
|||
Melt Flow | 80 g/10 min @Load 5.00 kg, Temperature 190 °C |
80 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
ELASTO UK Dryflex® 3039-201 TPE, Modified Injection Molding Grade for Sanitary Seals The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 3039-201 is specifically designe.. |
|||
Melt Flow | 80 g/10 min @Load 2.16 kg, Temperature 160 °C |
80 g/10 min @Load 4.76 lb, Temperature 320 °F |
cm<sup>3</sup>/10 min; ISO 1133 |
EMS-Griltech Griltex® D 1299A Heat Stabilized Copolyamide Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melt Flow | 80 g/10 min @Load 2.16 kg, Temperature 160 °C |
80 g/10 min @Load 4.76 lb, Temperature 320 °F |
cm<sup>3</sup>/10 min; ISO 1133 |
EMS-Griltech Griltex® D 1299A Heat Stabilized Copolyamide Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melt Flow | 80 g/10 min @Load 2.16 kg |
80 g/10 min @Load 4.76 lb |
Melt flow ratio I10/I2 is 8. |
Dow DOWLEX™ IP-2580 Linear Low Density Polyethylene Next Generation DOWLEX® IP-2580 resin is an improved processing linear low density polyethylene resin designed for excellent flow and stiffness with freezer grade impact properties. DOWLEX IP-2580 .. |
|||
Melt Flow | 80 g/10 min @Load 2.16 kg, Temperature 230 °C |
80 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238L |
Braskem H 107 Coating Polypropylene Description: H 107 is a ultra-high melt flow rate additivated homopolymer used for general purposes. Designed for extrusion coating. This product exhibits excellent processability, good melt stabili.. |
|||
Melt Flow | 80 g/10 min @Load 2.16 kg, Temperature 230 °C |
80 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238L |
Braskem H 107 Injection Molding Polypropylene Applications: Thin-walled parts and easy mould filling. Information provided by Braskem |
|||
Melt Flow | 80 g/10 min @Load 5.00 kg, Temperature 275 °C |
80 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
Azoty Tarnow™ Tarnamid® T-27 GB30 Polyamide 6 - Glass Beads Reinforced 30% Glass beads reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Melt Flow | 80 g/10 min @Load 2.16 kg, Temperature 230 °C |
80 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Braskem TI6800WV Impact Copolymer Polypropylene Description: High Melt Flow, Nucleated, Excellent Mold Release, AntistaticApplications: Suggested Uses Include Housewares, Large Part Injection Molding, Thin-Walled Injection MoldingThis resin meets.. |
|||
Melt Flow | 80 g/10 min @Load 5.00 kg, Temperature 275 °C |
80 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
BASF Ultramid® A27 E 01 PA66 (Conditioned) Ultramid A27 E 01 is a low-viscosity, general-purpose PA66 grade for compounding. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendation ".. |
|||
Melt Flow | 80 g/10 min @Load 5.00 kg, Temperature 275 °C |
80 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
BASF Ultramid® A27 E 01 PA66 (Dry) Ultramid A27 E 01 is a low-viscosity, general-purpose PA66 grade for compounding. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendation ".. |
|||
Melt Flow | 80 g/10 min @Load 2.16 kg, Temperature 230 °C |
80 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238L |
Braskem CP 191 Injection Molding Polypropylene Applications: Household; low temperature packing; frozen desserts packaging. Information provided by Braskem |
|||
Melt Flow | 80 g/10 min @Load 5.00 kg, Temperature 275 °C |
80 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
Azoty Tarnow™ Tarnamid® T-27 MW30 Polyamide 6 - Mineral Reinforced 30% Mineral filled, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High mechani.. |
|||
Melt Flow | 80 g/10 min @Load 5.00 kg, Temperature 275 °C |
80 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
BASF Ultramid® A3HG2 10% Glass Filled PA66 (Conditioned) Ultramid A 3HG2 is a 10% glass fiber reinforced grade of nylon 6/6 for injection molding. |
|||
Melt Flow | 80 g/10 min @Load 2.16 kg, Temperature 190 °C |
80 g/10 min @Load 4.76 lb, Temperature 374 °F |
"E"; ASTM D1238 |
Aaron Industries AAROPRENE® ATPR 1000 60A Elastomeric Compound AAROPRENE® ATPR 1000 Series Elastomeric CompoundDurometer values may be specified. Color may be specified. |
|||
Melt Flow | 80 g/10 min | 80 g/10 min | ASTM D1238 |
Huntsman PE2080 Injection Molding Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Very high flow rapid set-up characteristics, excellent clarity, and gloss.Applications: Injection molding: lids and difficult to fill applications.FDA Notes: .. |