Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 8.27 MPa | 1200 psi | ASTM D412 |
Polymax® Maxelast® P3855 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 8.27 MPa | 1200 psi | ASTM D412 |
Polymax® Maxelast® C4880 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Tensile Strength, Yield | 8.30 MPa | 1200 psi | 500 mm/min; ASTM D638 |
Eastman D4056-P Polyethylene
(discontinued **) Polyethylene D4056-P is a natural low density material with an 80 melt index.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no lon.. |
|||
Tensile Strength, Yield | 8.30 MPa | 1200 psi | |
Kraton® D1102 + LDPE blend (20/80) Blending KRATON D and G polymers with PE significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A.. |
|||
Tensile Strength, Yield | 8.27 MPa | 1200 psi | @100% Elongation; ASTM D1414 |
Greene Tweed CHEMRAZ® 661 Perfluoroelastomer Chemraz® 661 perfluoroelastomer is specifically developed by Greene Tweed to meet the unique demands of aggressive plasma systems. This product’s unique formulation provides enhanced plasma.. |
|||
Tensile Strength, Yield | 8.27 MPa | 1200 psi | Elastic; ASTM D412 |
Multibase Multi-Flex® A 5003 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Tensile Strength, Yield | 8.27 MPa | 1200 psi | Tensile strength decreases by 25% after dry heat aging for 70 hrs at 437°F.; ASTM D412 |
Saint-Gobain COHRlastic® 9275 High Performance Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
Tensile Strength, Yield | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex APEX® 3201-50 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |
|||
Tensile Strength, Yield | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex APEX® 3210-60 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge.. |
|||
Tensile Strength, Yield | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex APEX® 3301-50 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To.. |
|||
Tensile Strength, Yield | 8.27 MPa | 1200 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3302-80 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses- Medical Applications, Tubing, Appearance-ClearForms-PelletsProcessing-ExtrusionInformation provided by.. |
|||
Tensile Strength, Yield | 8.27 MPa | 1200 psi | 3; ASTM D412 |
Teknor Apex Flexalloy® 3501-50-NT Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MW, Ethylene Oxide SterilizableForms-PelletsProcessing-Extrusion, Injection MoldingAppe.. |
|||
Tensile Strength, Yield | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex MONPRENE® MP 2840M Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex MONPRENE® MP 2850E Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | >= 8.27 MPa | >= 1200 psi | Stress at Elongation M100; ASTM D412 Method A |
Seals Eastern 7157 Nitrile Rubber Nitrile for oil & gas serviceInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 8.27 MPa | 1200 psi | Tensile strength decreases by 20% after dry heat aging for 70 hrs at 437°F.; ASTM D412 |
Saint-Gobain COHRlastic® 9255 High Performance Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
Tensile Strength, Yield | 8.27 MPa | 1200 psi | ASTM D412-92 |
Saint-Gobain Versilicâ„¢ SPX-70I.B. High Strength Silicone Pressure Tubing Formulation Description: Versilicâ„¢ SPX-70 I.B.: Produced form a proprietary combination of silicone elastomers, Versilicâ„¢ SPX-70 I.B. Tubing optimizes critical physical properties such as tensile st.. |
|||
Tensile Strength, Yield | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex TEKBOND® 6000-60 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex TEKBOND® MP 1728 UVF Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 8.27 MPa @Temperature 21.1 °C |
1200 psi @Temperature 70.0 °F |
Flatwise Tensile |
Hexcel® Redux® 308A-NA Modified epoxy film adhesive Redux 308A-NA is a high-strength, flow-controlled film adhesive with flexible cure schedules at 300°F or 350°F. Redux 308A-NA contains glass beads that give good flow control. It is suitable for m.. |
|||
Tensile Strength, Yield | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex UNIPRENE® 7010-80 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 8.30 MPa | 1200 psi | ASTM D412 |
Elastocon TPE Technologies Elastocon® STK60X Thermoplastic Elastomer Elastocon® STK60X thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK60X is well suited for consume.. |
|||
Tensile Strength, Yield | 8.27 MPa | 1200 psi | Molded and tested in accordance with ASTM D4976; ASTM D638 |
Dow 722 Linear Low Density Polyethylene (LDPE) DOW Polyethylene 722 is a broad molecular weight distribution homopolymer designed to offer good impact strength and rack resistance, with excellent flexibility. Typical applications include caps/c.. |
|||
Tensile Strength, Yield | 8.30 MPa | 1200 psi | |
Dow AFFINITY™ SM 1350 Polyolefin Plastomer AFFINITY® SM 1350 polyolefin plastomer is an alpha-olefin resin that offers excellent performance in durable injection molded housewares and compression molded closure liners or gaskets. It exhibit.. |
|||
Tensile Strength, Yield | 8.30 MPa | 1200 psi | 508 mm/min; ASTM D638 |
Dow Engage® 8445 Polyolefin Elastomer Description: Engage® 8445 polyolefin elastomer is an ethyleneoctene copolymer that performs well in a wide range of thermoplastic elastomer applications. It has excellent compatibility with other p.. |
|||
Tensile Strength, Yield | 8.30 MPa | 1200 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers Softflex® 1701-1402 Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 8.27 MPa | 1200 psi | ASTM D-638 |
Axiall 8542 Moldings & Extrusions Flexible PVC General purpose, flexible PVC compound recommended for extrusion or molding applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 8.27 MPa | 1200 psi | ASTM D-638 |
Axiall 8554 Moldings & Extrusions Flexible PVC General purpose, jelly clear flexible PVC compound recommended for extrusion or molding applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 8.30 MPa | 1200 psi | 508 mm/min; ASTM D638 |
Dow Engage® 8540 Polyolefin Elastomer Description: Engage® 8540 polyolefin elastomer is an ethyleneoctene copolymer that is well suited to foamed applications and offers excellent performance for profile extrusion of tubing and hoses. .. |
|||
Tensile Strength, Yield | 8.27 MPa | 1200 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® IT 38-074 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerTransparentApplications:Hot Runner MoldingFDA (Food Contact)Teething ring & pacifierMulti-PurposeMarket:Consumer GoodsProcessing Method:I.. |