Category Polymer , Thermoplastic , Polyester, TP
Manufacturer Eastman Chemical
Trade Name Aspira
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman Aspira EB062 Copolyester Resin for Extrusion Blown Bottles.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Applications:Beverage packagingBottlesExtrusion blow moldingFood packagingPersonal care bottlesKey Attributes:Easy to extrude, cut, print and sealEffective barrier propertiesExcellent chemical resistanceExcellent clarityExcellent colorabilityGood impact strengthGood stiffnessHigh gloss appearanceToughnessProduct Description: Eastman Aspira copolyester EB062 is a resin specifically developed for extrusion blown bottles where aesthetics such as high clarity and gloss, coupled with design flexibility, drive demand. Compared to commonly used materials, Eastman Aspira copolyester EB062 runs on most standard processing equipment. Extremely high melt strength makes the resin an excellent choice when manufacturing large bottles.This product has been GREENGUARD INDOOR AIR QUALITY CERTIFIED®. This product is certified to NSF/ANSI Standard 51 for Food Equipment Materials. This product has been CRADLE TO CRADLE CERTIFIEDcm Silver.Information Provided by Eastman™
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength at Break 48.0 MPa
6960 psi
ASTM D638
Tensile Strength, Yield 47.0 MPa
6820 psi
ASTM D638
Elongation at Break 300 %
300 %
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Tensile Modulus 1.90 GPa
276 ksi
ASTM D638
Flexural Strength 65.0 MPa
9430 psi
ASTM D790
Flexural Modulus 1.90 GPa
276 ksi
ASTM D790
Izod Impact, Notched 0.630 J/cm

@Temperature -40.0 °C
1.18 ft-lb/in

@Temperature -40.0 °F
ASTM D256
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched NB

@Temperature -40.0 °C
NB

@Temperature -40.0 °F
ASTM D4812
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ASTM D4812
Puncture Energy 39.0 J

@Temperature -40.0 °C
28.8 ft-lb

@Temperature -40.0 °F
At Max load; ASTM D3763
41.0 J

@Temperature 23.0 °C
30.2 ft-lb

@Temperature 73.4 °F
At Max load; ASTM D3763
41.0 J

@Temperature 0.000 °C
30.2 ft-lb

@Temperature 32.0 °F
At Max load; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 73.0 °C
163 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 63.0 °C
145 °F
ASTM D648
Vicat Softening Point 85.0 °C
185 °F
ASTM D1525
Optical Properties Metric English Comments
Haze 1.3 %
1.3 %
ASTM D1003
Gloss 143 %
143 %
at 60°; ASTM D2457
Transmission, Visible 87 %
87 %
Regular; ASTM D1003
91 %
91 %
Total; ASTM D1003
Descriptive Properties Value Comments
Color -0.2
a*, ASTM D2244
0.6
b*, ASTM D2244
95
L*, ASTM D2244