Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 39.0 J @Temperature -40.0 °C |
28.8 ft-lb @Temperature -40.0 °F |
At Max load; ASTM D3763 |
Eastman Aspira EB062 Copolyester Resin for Extrusion Blown Bottles Applications:Beverage packagingBottlesExtrusion blow moldingFood packagingPersonal care bottlesKey Attributes:Easy to extrude, cut, print and sealEffective barrier propertiesExcellent chemical resis.. |