California Fine Wire Nickel Alloy 120 Nickel Iron Resistance Wire

Category Metal , Electronic/Magnetic Alloy , Nonferrous Metal , Nickel Alloy
Manufacturer California Fine Wire
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF California Fine Wire Nickel Alloy 120 Nickel Iron Resistance Wire.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Physical Properties Metric English Comments
Density 8.44 g/cc
0.305 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 483 MPa
70000 psi
Annealed
1030 MPa
150000 psi
Hard
Thermal Properties Metric English Comments
CTE, linear 15.0 µm/m-°C

@Temperature 20.0 °C
8.33 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 0.523 J/g-°C

@Temperature 20.0 °C
0.125 BTU/lb-°F

@Temperature 68.0 °F
Thermal Conductivity 28.9 W/m-K
201 BTU-in/hr-ft²-°F
Melting Point 1425 °C
2597 °F
Maximum Service Temperature, Air 1099 °C
2010 °F
Operating Temperature
Component Elements Properties Metric English Comments
Iron, Fe 30 %
30 %
Nickel, Ni 70 %
70 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000199 ohm-cm
0.0000199 ohm-cm
3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
Descriptive Properties Value Comments
Magnetic Strong
Temperature Coefficient of Resistance 0.0045 ohms/ohm-°C
0-100°C
Thermal EMF vs. Copper -0.04