Category Polymer , Thermoplastic , ABS Polymer , ABS/Polyester Alloy + GF , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer E-Polymers Co. Ltd.
Trade Name TEKALOY®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF E-Polymers Tekaloy® T80GFR , Flame Retardant, 30% Glass Fiber Reinforced PBT/ABS Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% Glass Fiber reinforced, Flame RetardantInformation provided by E-Polymers Co. Ltd.
Physical Properties Metric English Comments
Density 1.54 g/cc
0.0556 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D785
Tensile Strength, Yield 130 MPa
18900 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Yield Strength 160 MPa
23200 psi
ASTM D790
Flexural Modulus 8.20 GPa
1190 ksi
ASTM D790
Izod Impact, Notched 0.750 J/cm
1.41 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 202 °C
396 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 172 °C
342 °F
ASTM D648
Flammability, UL94 V-0
V-0
Processing Properties Metric English Comments
Processing Temperature 230 - 260 °C
446 - 500 °F
Mold Temperature 70.0 - 90.0 °C
158 - 194 °F