Material Notes:
Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding productivity. SEPAZ LCP has a unique attribute in that the thinner the product becomes, the greater the mechanical strength. SEPAZ LCP finds uses in connectors, sensors and other electronic components and CD pick-up parts, and in copying machine and fax components in office and audio-visual equipment.Information Provided by E-Polymers Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.74 g/cc
1.74 g/cc
ASTM D792
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
Mechanical Properties Metric English Comments
Tensile Strength 130.5 MPa
18920 psi
ASTM D638
Elongation at Break 1.5 %
1.5 %
ASTM D638
Flexural Strength 181.49 MPa
26323 psi
ASTM D790
Flexural Modulus 12.753 GPa
1849.7 ksi
ASTM D790
Izod Impact, Notched 0.392 J/cm
0.735 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 352 °C
666 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 300 °C
572 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 360 - 370 °C
680 - 698 °F
Mold Temperature 40.0 - 150 °C
104 - 302 °F