Polymer Property : Tensile Strength = 18920 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 130.5 MPa
18920 psi
ASTM D638
E-Polymers SEPAZ® C240GM 40% Glass Fiber/Mineral Reinforced LCP Resin
Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding ..