Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Zytel® PLS FR95G15DH2 BK269 Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 20% Glass Fiber Filled
Manufacturer DuPont Performance Polymers
Trade Name Zytel® PLS
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® PLS FR95G15DH2 BK269 Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
15% Glass Reinforced Flame Retardant Heat Stabilized Polyamide Zytel PLSFR95G15DH2 BK269 is 15% glass reinforced flame retardant black PA using SHIELD Technology only from DuPont exceptional resistance in hot airInformation provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
DAM; ISO 1183
Linear Mold Shrinkage, Flow 0.0040 cm/cm
0.0040 in/in
DAM; ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
0.0070 in/in
DAM; ISO 294-4 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 138 MPa
20000 psi
DAM; ISO 527-1/-2
Elongation at Break 2.6 %
2.6 %
DAM; ISO 527-1/-2
Tensile Modulus 7.35 GPa
1070 ksi
DAM; ISO 527-1/-2
Flexural Strength 197 MPa
28600 psi
DAM; ISO 178
Flexural Modulus 6.50 GPa
943 ksi
DAM; ISO 178
Charpy Impact Unnotched 3.90 J/cm²
18.6 ft-lb/in²
DAM; ISO 179/1eU
3.60 J/cm²

@Temperature -30.0 °C
17.1 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 179/1eU
Charpy Impact, Notched 0.640 J/cm²
3.05 ft-lb/in²
DAM; ISO 179/1eA
0.620 J/cm²

@Temperature -30.0 °C
2.95 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
DAM; 10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 258 °C
496 °F
DAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 237 °C
459 °F
DAM; ISO 75-1/-2
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
DAM; IEC 60695-11-10
V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
DAM; IEC 60695-11-10
Descriptive Properties Value Comments
Additives Release agent
Delivery Form Pellets
Part Marking Code >PA-GF15FR(17)<
ISO 11469
Processing Injection Moulding
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification PA-GF15FR(17)
Special Characteristics Heat stabilised or stable to heat