China Tungsten ZK10UF Tungsten Carbide

Category Ceramic , Carbide
Manufacturer China Tungsten
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF China Tungsten ZK10UF Tungsten Carbide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Semi-finishing and finishing of cast-irons and nonferrous metals it's also the unique material of solid carbide tools for holing.Information provided by China Tungsten
Physical Properties Metric English Comments
Density 14.8 g/cc
0.535 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell A 93
93
Flexural Strength 2000 MPa
290000 psi