Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)  (Unverified Data**)

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 50% Glass Fiber Reinforced
Manufacturer DuPont Performance Polymers
Trade Name Zytel® HTN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
45% Glass Reinforced Flame Retardant PPA High Performance Polyamide Zytel HTNFR52G45BL BK337 is a 45% glass reinforced flame retardant lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.76 g/cc
0.0636 lb/in³
DAM; ISO 1183
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
DAM; ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
DAM; ISO 294-4 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 155 MPa
22500 psi
50%RH; ISO 527-1/-2
175 MPa
25400 psi
DAM; ISO 527-1/-2
Elongation at Break 1.3 %
1.3 %
DAM; ISO 527-1/-2
1.5 %
1.5 %
50%RH; ISO 527-1/-2
Tensile Modulus 17.0 GPa
2470 ksi
DAM; ISO 527-1/-2
17.0 GPa
2470 ksi
50%RH; ISO 527-1/-2
Flexural Strength 260 MPa
37700 psi
50%RH; ISO 178
290 MPa
42100 psi
DAM; ISO 178
Flexural Modulus 15.2 GPa
2200 ksi
DAM; ISO 178
15.2 GPa
2200 ksi
50%RH; ISO 178
Izod Impact, Notched (ISO) 12.0 kJ/m²
5.71 ft-lb/in²
DAM; ISO 180/1A
Charpy Impact Unnotched 3.60 J/cm²
17.1 ft-lb/in²
50%RH; ISO 179/1eU
4.20 J/cm²
20.0 ft-lb/in²
DAM; ISO 179/1eU
3.60 J/cm²

@Temperature -30.0 °C
17.1 ft-lb/in²

@Temperature -22.0 °F
50%RH; ISO 179/1eU
4.00 J/cm²

@Temperature -30.0 °C
19.0 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 179/1eU
Charpy Impact, Notched 1.30 J/cm²
6.19 ft-lb/in²
DAM; ISO 179/1eA
1.30 J/cm²

@Temperature -40.0 °C
6.19 ft-lb/in²

@Temperature -40.0 °F
DAM; ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 15.0 µm/m-°C
8.33 µin/in-°F
DAM; ISO 11359-1/-2
8.00 µm/m-°C

@Temperature 55.0 - 160 °C
4.44 µin/in-°F

@Temperature 131 - 320 °F
DAM; ISO 11359-1/-2
15.0 µm/m-°C

@Temperature -40.0 - 23.0 °C
8.33 µin/in-°F

@Temperature -40.0 - 73.4 °F
DAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 50.0 µm/m-°C
27.8 µin/in-°F
DAM; ISO 11359-1/-2
50.0 µm/m-°C

@Temperature -40.0 - 23.0 °C
27.8 µin/in-°F

@Temperature -40.0 - 73.4 °F
DAM; ISO 11359-1/-2
75.0 µm/m-°C

@Temperature 55.0 - 160 °C
41.7 µin/in-°F

@Temperature 131 - 320 °F
DAM; ISO 11359-1/-2
Melting Point 310 °C
590 °F
DAM; first heat; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 300 °C
572 °F
DAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 284 °C
543 °F
DAM; ISO 75-1/-2
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
DAM; IEC 60695-11-10
V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
DAM; IEC 60695-11-10
Oxygen Index 49 %
49 %
DAM; ISO 4589-1/-2
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
DAM; IEC 60093
Dielectric Constant 3.6

@Frequency 1.00e+6 Hz
3.6

@Frequency 1.00e+6 Hz
DAM; IEC 60250
3.9

@Frequency 100 Hz
3.9

@Frequency 100 Hz
DAM; IEC 60250
Dielectric Strength 31.0 kV/mm
787 kV/in
DAM; IEC 60243-1
Dissipation Factor 0.0045

@Frequency 100 Hz
0.0045

@Frequency 100 Hz
DAM; IEC 60250
0.0112

@Frequency 1.00e+6 Hz
0.0112

@Frequency 1.00e+6 Hz
DAM; IEC 60250
Comparative Tracking Index 500 V
500 V
DAM; IEC 60112
Descriptive Properties Value Comments
Additives Lubricants
Release agent
Delivery Form Pellets
Part Marking Code >PA6T/66-GF45FR<
ISO 11469
>PPA-GF45FR<
SAE J1344
Processing Injection Moulding
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
UL recognition UL
DAM