Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527 Type 1A |
Solvay TECHNYLSTARâ„¢ AFX 218 V50 PA6, 50% glass filled, DRY Description TECHNYLSTARâ„¢ AFX 218 V50 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. It is availab.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527 Type 1A |
Solvay TECHNYLSTARâ„¢ SX 216 V50 PA6, 50% glass filled, DRY Description: TECHNYLSTAR Polyamide, reinforced with 50% of glass fiber, characterized by a high fluidity of the melt, for injection molding.Available in: Asia Pacific, Europe and North America Produ.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527 Type 1A |
Solvay TECHNYLSTARâ„¢ SX 218 V50 PA6, 50% glass filled, DRY Description: TECHNYLSTARâ„¢ SX 218 V50 is based on a patented high flow polyamide 6 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. This product i.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527-2 |
Solvay Specialty Polymers Ixef® 1025 Polyarylamide (PARA), 50% Glass Fiber Ixef® 1025 is a 50% glass-fiber reinforced, UV stabilized polyarylamide which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Features: Good Ch.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527-2 |
Solvay Specialty Polymers Kalix® 9945 HFFR Polyamide, High Performance (HPPA), 45% Glass Fiber Kalix® 9945 HFFR is a 45% glass-fiber reinforced, halogen-free flame retardant High Performance Polyamide. It is hot-water moldable and intended for use in components requiring superior mechanica.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527-2 |
Solvay Specialty Polymers Omnix® 4050 Polyamide, High Performance (HPPA) (Dry) Omnix® 4050 is a 50% glass-fiber reinforced, high-performance polyamide (HPPA). It is particularly suited for replacing die-cast metal in a variety of mechanical applications and components used .. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527-2 |
Solvay Specialty Polymers Omnix® FC-9050 Polyamide, High Performance (HPPA), 50% Glass Fiber Omnix® FC-9050 is a 50% glass-fiber reinforced high-performance polyamide. It is hot-water moldable and intended for use in components requiring superior mechanical properties even after moisture.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ASTM D638 |
Lubrizol Isoplast® 101LGF60NAT Engineering Thermoplastic Polyurethane Resin Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527 |
Vyncolit X620/1 Novolac Phenolic Glass fiber and graphite filled phenolic molding compound with excellent friction properties.USES: Low friction bearings, video recorder and compact disc parts. Not suitable for applications requir.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® 1SVX-65H black 9288 PA1010-GF65 Product Description: Grilamid 1SVX-65H black is a 65% glass fiber reinforced Polyamide 1010 injection molding grade with the following product profile: Raw materials based on renewable resources Exc.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527-1/-2 |
DSM Stanyl® TE250F9 (DAM) Nylon 46 45% Glass Reinforced, Heat Stabilized, Flame Retardant (North America) Information provided by DSM Engineering Plastics. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-5 FWA black 9225 PA*-GF50 Product description: Grivory GV-5 FWA black 9225 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copoly.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-5H PA*-GF50 Product description: Grivory GV-5H natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyamide.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-5HL black 9914 PA*-GF50 Product description: Grivory GV-5HL black 9914 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TSGL-60/4 black 9833 PA666-GF60 Product description: Grilon TSGL-60/4 black is based on a heat stabilized semicrystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 black is characterized by the following key-p.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527 |
Eurotec® Tecodur® PB70 GR50 BK009 MX01 PBT/PET, 50% glass fiber reinforced, heat & UV stabilized, improved impact, natural Information provided by Eurotec® |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GVL-5H black 9915 PA*-GF50 Product description: Grivory GVL-5H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H blac.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® GVS-5H black 9915 PA*-GF50 Product description: Grivory GVS-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam.. |
|||
Tensile Modulus | 17.0 GPa @Temperature 80.0 °C |
2470 ksi @Temperature 176 °F |
|
Akro-Plastic Akromid® T1 GF 50 (3101) PPA Dry, 50% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527-2 |
CENTROPLAST CENTROMID 6.6 CF 20 Polyamide 6.6 carbon fiber This material has very high strength and a high operating temperature. It can be used for precision components, drive parts and housings.Information provided by CENTROPLAST Engineering Plastics GMB.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® B3 GF 50 (2475) PA 6 Dry, 50% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527-1 |
Vyncolit Neopreg Kinel® SK60 L8G Glass Fiber Reinforced Molding Compound High flow, epoxy based molding compound long glass fiber reinforced with excellent long term property retention over a wide temperature range and climate conditions. It is particularly suited fo.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GVX-5 H nat PA*-GF50 Product description: Grivory GVX-5H natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamid.. |