Polymer Property : CTE, linear, Parallel to Flow = 8.00 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 8.00 µm/m-°C

@Temperature 20.0 °C
4.44 µin/in-°F

@Temperature 68.0 °F
ASTM E381
Solvay Specialty Polymers Kadel® E-1230 Polyketone  (discontinued **)
Electrical Conductor. High performance proprietary semi-crystalline polymer based resins with exceptional solvent resistance and high temperature performance. They provide strength and stiffness, p..
CTE, linear, Parallel to Flow 8.00 µm/m-°C

@Temperature -30.0 - 30.0 °C
4.44 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP EX03647H PEI
LNP LUBRICOMP* EX03647H is a compound based on Polyetherimide resin containing Proprietary Fillers. Added features of this material include: Healthcare, Wear Resistant.
CTE, linear, Parallel to Flow 8.00 µm/m-°C

@Temperature 23.0 - 60.0 °C
4.44 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Lubricomp UCL36AS PPA (Europe-Africa-Middle East)
LNP* LUBRICOMP* UCL36AS is a compound based on Polyphthalamide resin containing Carbon Fiber, PTFE. Added features include; Internally Lubricated, Electrically Conductive, Heat Stabilized.This data ..
CTE, linear, Parallel to Flow 8.00 µm/m-°C

@Temperature 23.0 - 60.0 °C
4.44 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP UCL36ASP PPA (Europe-Africa-Middle East)
LNP* LUBRICOMP* UCL36ASP is a compound based on Polyphthalamide resin containing Carbon Fiber, PTFE. Added features include; Internally Lubricated, Electrically Conductive, Heat Stabilized.
CTE, linear, Parallel to Flow 8.00 µm/m-°C

@Temperature 23.0 - 60.0 °C
4.44 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP RC006 PA6.6 (Europe-Africa-Middle East)
LNP* THERMOCOMP* RC006 is a compound based on PA6.6 resin containing Carbon Fiber. Added features include: Electrically Conductive.
CTE, linear, Parallel to Flow 8.00 µm/m-°C

@Temperature -30.0 - 30.0 °C
4.44 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP VERTON E9007E PEI
LNP* VERTON* E9007E is a compound based on Polyetherimide (PEI) containing 35% Long Carbon Fiber. Added features of this grade include: Structural, High Temperature
CTE, linear, Parallel to Flow 8.00 µm/m-°C

@Temperature -30.0 - 30.0 °C
4.44 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON OE006C1 PPS - Linear
LNP* STAT-KON* OE006C1 is a compound based on PPS - Linear resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.
CTE, linear, Parallel to Flow 8.00 µm/m-°C

@Temperature -30.0 - 30.0 °C
4.44 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON RE0069S PA 66
LNP* STAT-KON* RE0069S is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Heat Stabilized.
CTE, linear, Parallel to Flow 8.00 µm/m-°C
4.44 µin/in-°F
dry; ISO 11359-1/-2
DSM Stanyl® TW200B6 PA46-CF30
30% Carbon Reinforced, Heat Stabilized, Lubricated
CTE, linear, Parallel to Flow 8.00 µm/m-°C

@Temperature 150 °C
4.44 µin/in-°F

@Temperature 302 °F
ASTM E 228
DuPont Performance Polymers VESPEL TP-8556 Polyimide
Thermoplastic parts from filled PI (polyimide) for balanced mechanical properties and low wear and friction performance in high temperature hostile environmentsInformation provided by DuPont Perform..
CTE, linear, Parallel to Flow 8.00 µm/m-°C

@Temperature 55.0 - 160 °C
4.44 µin/in-°F

@Temperature 131 - 320 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)  (Unverified Data**)
45% Glass Reinforced Flame Retardant PPA High Performance Polyamide Zytel HTNFR52G45BL BK337 is a 45% glass reinforced flame retardant lubricated high performance polyamide resin that has been devel..
CTE, linear, Parallel to Flow 8.00 µm/m-°C
4.44 µin/in-°F
DIN 53752
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
CTE, linear, Parallel to Flow 8.00 µm/m-°C
4.44 µin/in-°F
DIN 53752
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
CTE, linear, Parallel to Flow 8.00 µm/m-°C
4.44 µin/in-°F
DIN 53752
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
CTE, linear, Parallel to Flow 8.00 - 9.00 µm/m-°C

@Temperature 23.0 - 80.0 °C
4.44 - 5.00 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 53752
BASF Ultradur® B 4300 G3 High Speed 15% Glass Filled PBT
Description: Is a PBT, easy-flowing injection-molding grades with 15% glass fibers; for rigid, tough and dimensionally stable technical parts.Applications: Housings, consoles, contact carriers, cove..
CTE, linear, Parallel to Flow 8.00 µm/m-°C
4.44 µin/in-°F
DIN 53752
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
CTE, linear, Parallel to Flow 8.00 µm/m-°C
4.44 µin/in-°F
DIN 53752
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
CTE, linear, Parallel to Flow 8.00 µm/m-°C
4.44 µin/in-°F
DIN 53752
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..