Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Zytel® FR95G25V0NH NC010 Nylon 66  (Unverified Data**)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer DuPont Performance Polymers
Trade Name Zytel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® FR95G25V0NH NC010 Nylon 66  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
25% Glass Reinforced Flame Retardant Polyamide 66 ZYTEL FR95G25V0NH NC010 is 25% glass fiber reinforced flame retardant polyamide halogen and red phosphorous free with high flow and excellent long term aging properties.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
DAM; ISO 1183
Water Absorption 4.0 %

@Thickness 2.00 mm
4.0 %

@Thickness 0.0787 in
DAM; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
DAM; ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
DAM; ISO 294-4 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 90.0 MPa
13100 psi
50%RH; ISO 527-1/-2
109 MPa
15800 psi
DAM; ISO 527-1/-2
Elongation at Break 2.2 %
2.2 %
DAM; ISO 527-1/-2
2.2 %
2.2 %
50%RH; ISO 527-1/-2
Tensile Modulus 8.70 GPa
1260 ksi
50%RH; ISO 527-1/-2
8.90 GPa
1290 ksi
DAM; ISO 527-1/-2
Charpy Impact Unnotched 3.10 J/cm²
14.8 ft-lb/in²
50%RH; ISO 179/1eU
3.50 J/cm²
16.7 ft-lb/in²
DAM; ISO 179/1eU
Charpy Impact, Notched 0.460 J/cm²
2.19 ft-lb/in²
DAM; ISO 179/1eA
0.450 J/cm²

@Temperature -30.0 °C
2.14 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 179/1eA
0.450 J/cm²

@Temperature -40.0 °C
2.14 ft-lb/in²

@Temperature -40.0 °F
DAM; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 267 °C
513 °F
DAM; 10°C/min; ISO 11357-1/-3
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
DAM; IEC 60695-11-10
V-0

@Thickness 0.400 mm
V-0

@Thickness 0.0157 in
DAM; IEC 60695-11-10
Electrical Properties Metric English Comments
Comparative Tracking Index 600 V
600 V
DAM; IEC 60112
Descriptive Properties Value Comments
Part Marking Code >PA-GF25FR<
ISO 11469
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification PA-GF25FR
ISO 1043
Temperature index tensile strength 160°C
IEC 60216-1; DAM; 20000hr
190°C
IEC 60216-1; DAM; 5000hr
UL recognition UL
DAM
Users viewing this material also viewed the following: