Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Delrin® 100T BK602 Acetal (POM)  (Unverified Data**)

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Homopolymer, Unreinforced, Impact Grade
Manufacturer DuPont Performance Polymers
Trade Name Delrin®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Delrin® 100T BK602 Acetal (POM)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Toughened High Viscosity Acetal Homopolymer Delrin 100T BK602 is a toughened high viscosity acetal homopolymer grade with superior impact resistance. It is designed for highly stressed parts where outstanding toughness is required.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ISO 1183
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 54.0 MPa
7830 psi
ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
Nominal; ISO 527-1/-2
Elongation at Yield 27 %
27 %
ISO 527-1/-2
Tensile Modulus 1.90 GPa
276 ksi
ISO 527-1/-2
Charpy Impact, Notched 2.30 J/cm²
10.9 ft-lb/in²
ISO 179/1eA
1.10 J/cm²

@Temperature -30.0 °C
5.23 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 178 °C
352 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C
160 °F
ISO 75-1/-2
Descriptive Properties Value Comments
Additives Lubricants
Release agent
Delivery Form Pellets
Emissions <8 mg/kg
VDA 275
Part Marking Code >POM-I<
ISO 11469
Processing Blow Moulding
Coatable
Injection Moulding
Other Extrusion
Profile Extrusion
Sheet Extrusion
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification POM-I
ISO 1043