Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | ISO179/3C DIN.53453 |
Omnia Plastica Omniamid PA6 G - G - at 50% RH Cast nylon 6. The method of production of this polyamide (i.e. the polymerisation of the caprolactam directly in the mould) allows the production of stock shapes in larger than normal dimensions, su.. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | ISO179/3C DIN.53453 |
Omnia Plastica Omniamid PA6 GHR - HR - at 50% RH Cast nylon 6 produced with the addition of graphite and a special lubricator which gives to this product better properties than natural PA6G. Whilst retaining the general features of OMNIAMID G it i.. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycolac® MG94 ABS (Europe-Africa-Middle East) Superior flow, injection molding ABS. Good impact. For thin-wall applications. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | ISO 179/1eA |
Iran Petrochemical (PCC) EX 3 - 80 High Density Polyethylene EX3-80 is a high density polyethylene with 1-Butene as co monomer. It is natural, good ESCR, good impact strength, tough and rigid pipe resin. Applications: pipe extrusion PE 80 class, industrial a.. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | ISO 179 |
Menzolit Menzolit® BMC 2300 Unsaturated Polyester UP BMC 2300 is a special BMC with exceptional high fire retardancy. The glass content is set to a level that provides sufficient mouldability with high strength and stiffness properties. Fire retardanc.. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® A 218HP V50 PA66, 35% glass fiber, Conditioned Description: TECHNYL® A 218HP V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: The product off.. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | 80*10*4mm, Cut; ISO 179/1eA |
SABIC Innovative Plastics Valox® V8030CS PBT+PET Glass filled Valox with enhanced surface |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC (Asia Pacific) Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen.. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL GTX GTX942 PPE+PS+PA66 Noryl GTX* GTX942 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is designed to have high melt flow for large part/thinwall injection molding. The material is designed to h.. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | ISO 179/1eA |
Borealis Nepol™ GB303HP 30% Long Glass Fiber Reinforced Polypropylene Nepol GB303HP is a 30% long glass fiber reinforced polypropylene grade, produced using Borealis ` propriety and exclusive, patented Nepol technology intended for injection molding and extrusion. Th.. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | ISO 179-1 |
Unitika EX-1020K PA6, Conditioned Conducting nylonInformation provided by Unitika Ltd. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | Bayer Test |
Covestro Baydur® 730 IBS Polyurethane Structural Foam RIM, Density 40 pcf, MDI-based 2-Component Liquid System 0.25 in. thickness. IBS = Interactive Blowing System RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience .. |
|||
Charpy Impact, Notched | 2.30 J/cm² @Temperature 23.0 °C |
10.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 GV 20 HWCP 20% Glass Fiber Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Delrin® 100T BK602 Acetal (POM)
(Unverified Data**) Toughened High Viscosity Acetal Homopolymer Delrin 100T BK602 is a toughened high viscosity acetal homopolymer grade with superior impact resistance. It is designed for highly stressed parts where o.. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | 50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® 73G30HSL BK416 Nylon 6
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G30HSL BK416 is a 30% glass fiber reinforced heat stabilized lubricated black polyamide 6 resin for injection molding.Information provided by.. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | 50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® 73G30L NC010 Nylon 6
(Unverified Data**) 30% Glass Reinforced Polyamide 6Zytel 73G30L NC010 is a 30% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® 80G43HS1L BK104 Nylon 66
(Unverified Data**) 43% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G43HS1L BK104 is a 43% glass fiber reinforced heat stabilized black polyamide 66 resin with superior impact resistance.Information.. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | After conditioning at 23°C/50%RH; ISO 179/Af |
Arkema Group Orgalloy® LE60 THM Polyamide Alloy Polyamide Alloy, Semi-Flexible gradeTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Charpy Impact, Notched | 2.30 J/cm² @Temperature -20.0 °C |
10.9 ft-lb/in² @Temperature -4.00 °F |
Dry; ISO 179/Af |
Arkema Group Orgalloy® RS 60E10 Polyamide Alloy Polyamide Alloy, Rigid Blown film gradeTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Charpy Impact, Notched | 2.30 J/cm² @Temperature 23.0 °C |
10.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Akro-Plastic Akromid® A3 GF 50 (2423) PA 6.6 Conditioned, 50% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Charpy Impact, Notched | 2.29 J/cm² | 10.9 ft-lb/in² | |
Arkema Group Rilsan® AZM 50 NOIR T6LD Nylon 12, 50% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-090,GF50Rigid grade with glass fiber (50%) for injection molding. Available color: black. Reinforced light and heat stabilizing agent. Mold-release agent.High rigid.. |
|||
Charpy Impact, Notched | 2.30 J/cm² @Temperature 23.0 °C |
10.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Akro-Plastic Akromid® B3 GF 40 (2474) PA 6 Conditioned, 40% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | ISO 179 |
BASF Ultramid® TG7S 35% Glass Filled PA6 (Dry) Ultramid TG7S is a 34% glass reinforced, heat stabilized, impact modified PA6 injection molding grade. It was developed to meet the demanding requirements of the first North American seat
cushion .. |